Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

LyondellBasell Alathon® H5618 High Density Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Injection Molded
Manufacturer LyondellBasell (former Equistar)
Trade Name Alathon®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LyondellBasell Alathon® H5618 High Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
ApplicationsALATHON H 5618 provides easy processing characteristics and exhibits excellent toughness properties and color as well as low odor and good processing stability. Typical applications include housewares, containers, caps and closures.Regulatory StatusH 5618 meets the requirements of Food and Drug Administration regulation, 21 CFR 177.1520. This regulation allows the use of this olefin polymer in "…articles or components of articles intended for use in contact with food." Specific limitations or conditions of use may apply. Contact your Equistar sales representative for more information. Processing TechniquesSpecific recommendations for processing H 5618 can only be made when the processing conditions, equipment and end use are known. For further suggestions, please contact your Equistar sales representative.This product is from the former Equistar product line.
Physical Properties Metric English Comments
Density 0.956 g/cc
0.0345 lb/in³
ASTM D1505
Melt Flow 18 g/10 min
18 g/10 min
ASTM D1238
Spiral Flow 33.0 cm
13.0 in
Measures the number on inches of flow produced when molten resin is injected into a long, spiral channel (0.625" insert), at a constant injection pressure of 1000 psi with a melt temperature of 440° F; Equistar
Mechanical Properties Metric English Comments
Hardness, Shore D 69
69
ASTM D2240
Tensile Strength at Break 27.6 MPa
4000 psi
ASTM D638
Tensile Strength, Yield 29.0 MPa
4210 psi
Crosshead speed - 2"min.; ASTM D638
Elongation at Yield 7.7 %
7.7 %
Crosshead speed - 2"min.; ASTM D638
1% Secant Modulus 1376 MPa
199600 psi
Crosshead speed - 0.5" min; ASTM D790
2% Secant Modulus 1.15 GPa
167 ksi
Crosshead speed - 0.5" min; ASTM D790
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 75.0 °C
167 °F
ASTM D648
Vicat Softening Point 125 °C
257 °F
ASTM D1525
Brittleness Temperature <= -76.0 °C
<= -105 °F
F<sub>50</sub>; ASTM D746
Users viewing this material also viewed the following: