Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Samsung Cheil Industries Starex® HF-0660I ABS, Unreinforced

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Molded
Manufacturer Samsung, Cheil Industries
Trade Name Starex®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Samsung Cheil Industries Starex® HF-0660I ABS, Unreinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Material with high flowability and high stiffness that can be used for vacuum cleaner, telephone, TV, VCR, calculator, radio and air-conditionerInformation provided by Samsung Cheil Industries.
Physical Properties Metric English Comments
Specific Gravity 1.04 g/cc
1.04 g/cc
ASTM D792
Melt Flow 3.3 g/10 min

@Load 5.00 kg,
Temperature 200 °C
3.3 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 109
109
ASTM D785
Tensile Strength, Yield 39.2 MPa
5690 psi
5 mm/min; ASTM D638
Flexural Strength 58.8 MPa
8530 psi
2.8 mm/min; ASTM D790
Flexural Modulus 2.16 GPa
313 ksi
2.8 mm/min; ASTM D790
Izod Impact, Notched 1.96 J/cm

@Thickness 6.35 mm
3.67 ft-lb/in

@Thickness 0.250 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 84.0 °C

@Thickness 6.40 mm
183 °F

@Thickness 0.252 in
ASTM D648
Vicat Softening Point 92.0 °C
198 °F
B/50; ISO R306