Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Samsung Cheil Industries Starex® SD-0170 ABS, Unreinforced

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Molded
Manufacturer Samsung, Cheil Industries
Trade Name Starex®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Samsung Cheil Industries Starex® SD-0170 ABS, Unreinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Samsung Cheil Industries.
Physical Properties Metric English Comments
Specific Gravity 1.03 g/cc
1.03 g/cc
ASTM D792
Melt Flow 11.5 g/10 min

@Load 10.0 kg,
Temperature 220 °C
11.5 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 95
95
ASTM D785
Tensile Strength, Yield 31.4 MPa
4550 psi
5 mm/min; ASTM D638
Flexural Strength 51.0 MPa
7400 psi
2.8 mm/min; ASTM D790
Flexural Modulus 1.67 GPa
242 ksi
2.8 mm/min; ASTM D790
Izod Impact, Notched 3.43 J/cm

@Thickness 6.35 mm
6.43 ft-lb/in

@Thickness 0.250 in
ASTM D256
Thermal Properties Metric English Comments
Vicat Softening Point 94.0 °C
201 °F
B/50; ISO R306