Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Sanyo PELESTAT® NC6321 ABS (12wt%)

Category Polymer , Thermoplastic
Manufacturer Sanyo Chemical Industries
Trade Name PELESTAT®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Sanyo PELESTAT® NC6321 ABS (12wt%).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PELESTAT® alloy type anti-static additives are true IDP (Inherent Dissipative Polymers) that give permanent static dissipation performance to thermoplastics. Pelestat® comes tailored to a variety of thermoplastics like polyolefins, ABS, PC/ABS, PS, HIPS, Acetal Nylon, PBT, PTEG, etc. Pelestat® is not affected by moisture or humidity and offers the highest heat resistance of any anti-stats without affecting mechanical properties of the thermoplastic.Information provided by Tomen America, a US distributor of Pelestat.
Physical Properties Metric English Comments
Melt Flow 30 g/10 min

@Load 10.0 kg,
Temperature 220 °C
30 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 41.0 MPa
5950 psi
Flexural Modulus 2.20 GPa
319 ksi
Izod Impact, Notched 1.40 J/cm
2.62 ft-lb/in
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 89.00 °C
192.2 °F
Electrical Properties Metric English Comments
Surface Resistance 2.00e+11 ohm
2.00e+11 ohm
Copyright © lookpolymers.com All Rights Reserved