Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.40 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
2.62 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Compression Molded, Flow; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Extrusion L0313 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Izod Impact, Notched | 1.40 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
2.62 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Nymax™ GF 600 A 44 Black 13 Polyamide 6 (Nylon 6) The Nymax® GF 600 Series of glass fiber-reinforced nylon 6 compounds have been specifically engineered for applications requiring high stiffness, tensile strength, and toughness, while providing en.. |
|||
Izod Impact, Notched | 1.40 J/cm @Temperature -30.0 °C |
2.62 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® FXD103R PC (Asia Pacific) FXD103R is a Light Diffusion effect, which is part of the VisualFX family. These effects have been developed to meet increasing Aesthetic demands in the Marketplace. Color Package may affect propert.. |
|||
Izod Impact, Notched | 1.40 J/cm @Temperature -30.0 °C |
2.62 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® FXD103R PC (Europe-Africa-Middle East) FXD103R is a Light Diffusion effect, which is part of the VisualFX family. These effects have been developed to meet increasing Aesthetic demands in the Marketplace. Color Package may affect propert.. |
|||
Izod Impact, Notched | 1.40 J/cm @Thickness 6.35 mm, Temperature 23.0 °C |
2.62 ft-lb/in @Thickness 0.250 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Edgetek® NN-50GF/000EM L Polyamide 66 (Nylon 66) Information provided by PolyOne |
|||
Izod Impact, Notched | 1.40 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
2.62 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Nymax™ GF 1200 A 55 HS Black 13 Polyamide 66 (Nylon 66) The Nymax® GF 1200 Series of glass fiber-reinforced nylon 6/6 compounds have been specifically formulated for applications requiring high stiffness, tensile properties, heat resistance, and durabil.. |
|||
Izod Impact, Notched | 1.40 J/cm | 2.62 ft-lb/in | |
Shell Carilon® DB6G6A10 Polyketone, 30% Glass-Reinforced General-Purpose Injection Molding Grade
(discontinue Shell announced in Feb. 2000 that the Carilon product line is being discontinued. CARILON Polymer DB6G6A10 is a 30 percent short glass-fiber-reinforced, general purpose injection molding grade, wit.. |
|||
Izod Impact, Notched | 1.40 J/cm @Temperature -30.0 °C |
2.62 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® FXD104R PC (Asia Pacific) FXD104R is a Light Diffusion effect, which is part of the VisualFX family. Color Package may affect properties. |
|||
Izod Impact, Notched | 1.40 J/cm @Temperature 0.000 °C |
2.62 ft-lb/in @Temperature 32.0 °F |
ASTM D256 |
Gichem GILAC E200 Acrylonitrile Butadiene Styrene
(discontinued **) ABS medium fluidity, excellent resilience. Medium-High Injection speed.Information provided by GICHEM Gruppo Industriale Chimico |
|||
Izod Impact, Notched | 1.40 J/cm | 2.62 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Torlon® 4203L Polyamide-imide (PAI)
(Unverified Data**) Torlon 4203L is an unreinforced, lubricated, pigmented grade of polyamide-imide (PAI) resin. It has the best impact resistance and greatest elongation of all the Torlon grades. Torlon PAI has the hi.. |
|||
Izod Impact, Notched | 1.40 J/cm @Temperature 23.0 °C |
2.62 ft-lb/in @Temperature 73.4 °F |
DAM; ASTM D256 |
DuPont Performance Polymers Zytel® 8018HS BKB085 Nylon 66
(Unverified Data**) Zytel® 8018HS BKB085 is a 14% glass reinforced, toughened, heat stabilized black polyamide 66 resin.Information provided by DuPont Performance Polymers |
|||
Izod Impact, Notched | 1.40 J/cm | 2.62 ft-lb/in | ASTM D256-03 |
Ipiranga Petrochem PH 0130 Polypropylene The production of polypropylene (PP) employs Spheripol technology from Montell / Italy. This technology has been acclaimed all over the world and is known as clean technology, because it does not pr.. |
|||
Izod Impact, Notched | 1.40 J/cm | 2.62 ft-lb/in | ASTM D256-03 |
Ipiranga Petrochem PH 0130 Polypropylene The production of polypropylene (PP) employs Spheripol technology from Montell / Italy. This technology has been acclaimed all over the world and is known as clean technology, because it does not pr.. |
|||
Izod Impact, Notched | 1.40 J/cm | 2.62 ft-lb/in | BS 2782.306A |
Micropol Isoplas P501 Crosslinkable Polyethylene Information provided by Micropol Limited |
|||
Izod Impact, Notched | 1.40 J/cm @Temperature -20.0 °C |
2.62 ft-lb/in @Temperature -4.00 °F |
BS 2782.306A |
Micropol Isoplas P501 Crosslinkable Polyethylene Information provided by Micropol Limited |
|||
Izod Impact, Notched | 1.40 J/cm | 2.62 ft-lb/in | ASTM D256 |
Loxim 330 01HSL Nylon 6 Information provided by Loxim Industries |
|||
Izod Impact, Notched | 1.40 J/cm | 2.62 ft-lb/in | ASTM D256-03 |
Ipiranga Petrochem GF 5150 HDPE IPQ produces High Density Polyethylene (HDPE) for use by different segments of the plastics molding industry in several processes, including blow molding, extrusion and injection molding.To produce .. |
|||
Izod Impact, Notched | 1.40 J/cm | 2.62 ft-lb/in | 63.5*12.7*3.2mm, Cut; ASTM D256 |
SABIC Innovative Plastics SABIC PPCOMPOUND 55T1030 PP SABIC® PPcompound 55T1030 is a general purpose, talc filled, heat stabilized copolymer polypropylene compound. This compound exhibits very high impact, and is suitable for multiple processing met.. |
|||
Izod Impact, Notched | 1.40 J/cm | 2.62 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Torlon® 4200 Polyamide-imide (PAI) Torlon® 4200 is an unreinforced, unpigmented grade of polyamide-imide (PAI) resin for extrusion. This grade is designed for applications in the semiconductor industry which cannot tolerate partic.. |
|||
Izod Impact, Notched | 1.40 J/cm | 2.62 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP D451 PC (Asia Pacific) LNP* Thermocomp* D451 (or EXTC8141) is a compound based on Polycarbonate resin containing Glass Fiber, Flame Retardant. Added features of this material include: High modulus, good flatness, good duc.. |
|||
Izod Impact, Notched | 1.40 J/cm | 2.62 ft-lb/in | ASTM D265 |
Solvay TECHNYL® 2412GHF8 PA66, 40% glass fiber, DRY Description: Polyamid 66, reinforced with 40% of glass fiber, heat stabilized for injection moldingAvailable in: Asia PacificProduct Applications: TECHNYL® 2412GHF8 is used in all sectors of indu.. |
|||
Izod Impact, Notched | 1.40 J/cm | 2.62 ft-lb/in | ISO 180 |
Wellman Wellamid® GF33-66/6 XE-N 33% Glass Fiber Reinforced Nylon 66/6, Lubricated & Heat Stabilized Typical Applications: Machinery gear trains and linkage, conveyor belt links, fasteners, auto under hood and door parts, automotive door handles, appliance parts, sporting goods, lawn and garden equ.. |
|||
Izod Impact, Notched | 1.40 J/cm @Temperature 23.0 °C |
2.62 ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
Polyram RamOfin PPH307G6 Polypropylene, 30% Glass Fiber 30% glass fiber reinforced, impact modified polypropylene for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Izod Impact, Notched | 1.40 J/cm | 2.62 ft-lb/in | ISO 180 |
Azoty Tarnow™ TARFLEN SM-2 PTFE Non Free Flowing suspension powder for standard compression molding and compounding.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Izod Impact, Notched | 1.40 J/cm | 2.62 ft-lb/in | ISO 180 |
Azoty Tarnow™ TARFLEN ST PTFE Free-Flowing suspension powder for ram extrusion of rods, pipes and other profiles.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Izod Impact, Notched | 1.40 J/cm | 2.62 ft-lb/in | ASTM D256 |
Adell BT-17 Nylon 6, 35% Glass Reinforced; Impact Modified Data provided by Adell Plastics, Inc. |
|||
Izod Impact, Notched | 1.40 J/cm | 2.62 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Torlon® 4203 Polyamide-imide (PAI)
(discontinued **) Torlon 4203 is an unreinforced, lubricated, pigmented grade of polyamide-imide (PAI) resin for extrusion. It has the best impact resistance and greatest elongation of all the Torlon grades. Torlon P.. |
|||
Izod Impact, Notched | 1.40 J/cm @Temperature -30.0 °C |
2.62 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® SLX2071T PC Copolymer (Europe-Africa-Middle East) High viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in transparent and tinted colors |