Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

TSE Industries Millathane® 5004 Millable Polyurethane Elastomer with 80 PHR N330 (HAF) Black

Category Polymer , Thermoset , Polyester, TS , Polyurethane, TS , Thermoset Polyurethane, Elastomer, Unreinforced , Rubber or Thermoset Elastomer (TSE)
Manufacturer TSE Industries, Inc
Trade Name Millathane®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF TSE Industries Millathane® 5004 Millable Polyurethane Elastomer with 80 PHR N330 (HAF) Black.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is carried out by the use of various peroxides including dicumyl peroxide (DCP) or 2,5-dimethyl-2,5-bis (t-butylperoxy) hexane (DBPH).FormulationMillathane 5004100Stearic Acid0.25N330 (HAF) Black80Di-Cup 40C6.0All information provided by TSE Industries
Mechanical Properties Metric English Comments
Hardness, Shore A 90
90
98
98
heat aged 70 hours at 300ºF
98
98
heat aged one week at 300ºF
Tensile Strength, Yield 9.79 MPa
1420 psi
heat aged one week at 300ºF
10.0 MPa
1450 psi
heat aged 70 hours at 300ºF
15.9 MPa
2310 psi
Elongation at Yield 50 %
50 %
heat aged 70 hours at 300ºF
60 %
60 %
heat aged one week at 300ºF
200 %
200 %
100% Modulus 0.0114 GPa
1.66 ksi
200% Modulus 0.0159 GPa
2.31 ksi
Processing Properties Metric English Comments
Cure Time 30.0 min

@Temperature 152 °C
0.500 hour

@Temperature 305 °F