Schott N-SF1 Glass

Category Ceramic , Glass
Manufacturer Schott North America
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Schott N-SF1 Glass.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information Provided by SCHOTT North America, Inc.
Physical Properties Metric English Comments
Density 3.03 g/cc
0.109 lb/in³
Mechanical Properties Metric English Comments
Knoop Microhardness 540
540
.1/20
Modulus of Elasticity 90.0 GPa
13100 ksi
Poissons Ratio 0.25
0.25
Shear Modulus 36.0 GPa
5220 ksi
calculated
Thermal Properties Metric English Comments
CTE, linear 9.10 µm/m-°C

@Temperature -30.0 - 70.0 °C
5.06 µin/in-°F

@Temperature -22.0 - 158 °F
10.5 µm/m-°C

@Temperature 20.0 - 300 °C
5.83 µin/in-°F

@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.750 J/g-°C
0.179 BTU/lb-°F
Thermal Conductivity 1.00 W/m-K
6.94 BTU-in/hr-ft²-°F
Transformation Temperature, Tg 553 °C
1030 °F
Optical Properties Metric English Comments
Refractive Index 1.71736

@Wavelength 587.6 nm
1.71736

@Wavelength 587.6 nm
n<sub>d</sub>
1.72308

@Wavelength 546.1 nm
1.72308

@Wavelength 546.1 nm
n<sub>e</sub>
Transmission, Visible 57.4 %

@Thickness 10.0 mm,
Wavelength 380 nm
57.4 %

@Thickness 0.394 in,
Wavelength 380 nm
89.6 %

@Thickness 10.0 mm,
Wavelength 405 nm
89.6 %

@Thickness 0.394 in,
Wavelength 405 nm
97.6 %

@Thickness 10.0 mm,
Wavelength 460 nm
97.6 %

@Thickness 0.394 in,
Wavelength 460 nm
99.6 %

@Thickness 10.0 mm,
Wavelength 580 nm
99.6 %

@Thickness 0.394 in,
Wavelength 580 nm
99.6 %

@Thickness 10.0 mm,
Wavelength 700 nm
99.6 %

@Thickness 0.394 in,
Wavelength 700 nm
IR Transmittance 77.3 %

@Thickness 10.0 mm,
Wavelength 2500 nm
77.3 %

@Thickness 0.394 in,
Wavelength 2500 nm
98.9 %

@Thickness 10.0 mm,
Wavelength 1530 nm
98.9 %

@Thickness 0.394 in,
Wavelength 1530 nm
UV Transmittance 9.6 %

@Thickness 10.0 mm,
Wavelength 365 nm
9.6 %

@Thickness 0.394 in,
Wavelength 365 nm
25.2 %

@Thickness 10.0 mm,
Wavelength 370 nm
25.2 %

@Thickness 0.394 in,
Wavelength 370 nm
Chemical Properties Metric English Comments
Acid Class, SR 1.0
1.0
Alkali Class, AR 1.0
1.0
Stain Resistance Class, FR 0.00
0.00
Descriptive Properties Value Comments
B 1
Climatic Resistance Test CR 1
HG 5
K (10-6mm2/N) 2.72
Phosphate Resistance PR 1
T1013.0 (°C) 554
T107.6 (°C) 660