Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 0.750 J/g-°C | 0.179 BTU/lb-°F | |
Osprey Metals CE7 Al-Si Controlled Expansion Alloy Si-30%Al controlled expansion alloy manufactured and patented by Osprey Metals Ltd.Information provided to MatWeb by Osprey Metals. |
|||
Specific Heat Capacity | 0.750 J/g-°C | 0.179 BTU/lb-°F | |
Schott N-SF1 Glass Information Provided by SCHOTT North America, Inc. |
|||
Specific Heat Capacity | 0.750 J/g-°C | 0.179 BTU/lb-°F | |
Schott N-SF14 Glass Information Provided by SCHOTT North America, Inc. |
|||
Specific Heat Capacity | 0.750 J/g-°C | 0.179 BTU/lb-°F | |
Saint-Gobain HS Grade Optical Fused Quartz HS Grade Optical Fused Quartz is a high purity, low [OH] natural fused quartz. It has excellent IR transmission, useful transmission from 260 to 3500 nm, excellent visual quality with low bubbles, .. |
|||
Specific Heat Capacity | 0.750 J/g-°C | 0.179 BTU/lb-°F | |
Saint-Gobain Quartzel® Fused Quartz Textiles Quartzel® fiber is produced from quartz crystal that is ground, purified, fiberized by a fusion process. It is homogeneous, non-porous, continuous, amorphous, ultra pure silica glass. It is ava.. |
|||
Specific Heat Capacity | 0.750 J/g-°C | 0.179 BTU/lb-°F | |
Saint-Gobain Spectrosil® 1000 Optical Fused Quartz Spectrosil® 1000 grade is used for non-transmissive mirrors and substrates, and other high purity components which do not require specified optical transmission.Spectrosil® is a synthetic fuse.. |
|||
Specific Heat Capacity | 0.750 J/g-°C | 0.179 BTU/lb-°F | |
Saint-Gobain Spectrosil® 2000 Optical Fused Quartz Spectrosil® 2000 is a deep UV, fluorescence-free grade.Spectrosil® is a synthetic fused silica manufactured using a patented, environmentally friendly process that results in a virtually chlor.. |
|||
Specific Heat Capacity | 0.750 J/g-°C | 0.179 BTU/lb-°F | |
Saint-Gobain Spectrosil® 2100 Optical Fused Quartz Spectrosil® 2100 has improved refractive index homogeneity.Spectrosil® is a synthetic fused silica manufactured using a patented, environmentally friendly process that results in a virtually c.. |
|||
Specific Heat Capacity | 0.750 J/g-°C | 0.179 BTU/lb-°F | |
Saint-Gobain Spectrosil® 2200 Optical Fused Quartz Spectrosil® 2200 grade is an excimer laser grade developed for maximum transmission and prolonged life in microlithography and other critical deep UV applications using KrF (248 nm) and ArF (193 .. |
|||
Specific Heat Capacity | 0.750 J/g-°C | 0.179 BTU/lb-°F | |
Saint-Gobain Vitreosil® 055 Optical Fused Quartz Vitreosil® 055 is the highest grade of optical grade fused quartz available from Saint-Gobain Quartz for use in the near UV and visible. It has a useful transmission range from 270 nm in the nea.. |
|||
Specific Heat Capacity | 0.750 J/g-°C | 0.179 BTU/lb-°F | |
Saint-Gobain Vitreosil® 065 066 Optical Fused Quartz Vitreosil® 065, for use in the near UV and visible, has a less rigorous bubble specification. It has a useful transmission range from 270 nm in the near UV to 2000 nm in the IR.Vitreosil® opt.. |
|||
Specific Heat Capacity | 0.750 J/g-°C | 0.179 BTU/lb-°F | |
Saint-Gobain Vitreosil® Clear Fused Quartz Tubing Electrically fused quartz is recognized for its combination of purity, chemical inertness, physical stability, thermal shock resistance, high electrical resistivity, and high operating temperatures... |
|||
Specific Heat Capacity | 0.750 J/g-°C | 0.179 BTU/lb-°F | |
Saint-Gobain Puropsil® B Infrared Grade Low [OH] Optical Fused Quartz Puropsil® B optical infrared fused quartz is manufactured from naturally occurring quartz crystal using a plasma process to ensure a low OH. It has excellent IR transmission with a useful IR tra.. |
|||
Specific Heat Capacity | 0.750 J/g-°C | 0.179 BTU/lb-°F | |
Saint-Gobain Vitreosil® CFQ/TSC Optical Fused Quartz Vitreosil® CFQ/TSC grades are for use in less demanding applications including viewing windows for use in corrosive and high temperature environments and non-optical components such as spacers, i.. |
|||
Specific Heat Capacity | 0.750 J/g-°C | 0.179 BTU/lb-°F | |
Goodfellow Ruby, Al2O3 Ruby exhibits identical properties to those of sapphire. Small amounts of impurities, especially chromium oxide, give ruby a red coloration. Useful optical range from 150 - 5500 nm.Information pro.. |
|||
Specific Heat Capacity | 0.750 J/g-°C | 0.179 BTU/lb-°F | |
Corning Vycor® 7913 UV-Transmitting Glass Special Features:Superior optical qualityTight dimensional controlThermal and chemical properties ideally suited to high temperatures.Excellent thermal shock resistanceTypical Applications:Halogen l.. |
|||
Specific Heat Capacity | 0.750 J/g-°C | 0.179 BTU/lb-°F | |
Corning Vycor® 7950 Red Glass Used to reduce the light of quartz lamps (blocks most visible white light while transmitting IR). One specific use is blocking glare from heating units.Special Features:Superior optical qualityTigh.. |
|||
Specific Heat Capacity | 0.750 J/g-°C @Temperature 50.0 °C |
0.179 BTU/lb-°F @Temperature 122 °F |
|
COI Ceramics Sylramic™ Crystalline Silicon Carbide (SiC) Fiber Description: Sylramic™ SiC fiber is a textile grade continuous tow (yarn) made up of 800 filaments with a denier of 1600. Each filament is 10µm in diameter and is coated with a polyvinyl alcohol (.. |