Material Notes:
Fluoro-siliconeInformation provided by Seals Eastern, Inc.
Mechanical Properties Metric English Comments
Hardness, Shore A >= 53
>= 53
ASTM D2240, Type A
61
61
AVG; ASTM D2240, Type A
Tensile Strength at Break >= 11.0 MPa
>= 1590 psi
ASTM D412 Method A
11.2 MPa
1630 psi
AVG; ASTM D412 Method A
Tensile Strength, Yield 0.965 MPa
140 psi
AVG Stress at Elongation M25; ASTM D412 Method A
>= 1.38 MPa
>= 200 psi
Stress at Elongation M50; ASTM D412 Method A
1.49 MPa
216 psi
AVG Stress at Elongation M50; ASTM D412 Method A
>= 2.45 MPa
>= 356 psi
Stress at Elongation M100; ASTM D412 Method A
2.54 MPa
369 psi
AVG Stress at Elongation M100; ASTM D412 Method A
Elongation at Break >= 320 %
>= 320 %
ASTM D412 Method A
325 %
325 %
AVG; ASTM D412 Method A
Modulus of Elasticity 0.00528 GPa
0.766 ksi
ASTM D412 Method A
Shear Modulus 0.00193 GPa
0.280 ksi
ASTM D412 Method A
Secant Modulus 0.00512 GPa
0.743 ksi
ASTM D412 Method A
Thermal Properties Metric English Comments
Glass Transition Temp, Tg -51.1 °C
-60.0 °F
ASTM D1329
Descriptive Properties Value Comments
Strain Energy / Unit Volume at 20% Elongation (psi) 14