Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | -20.0 °C | -4.00 °F | DSC |
3M Dyneon™ Fluorel™ Dipolymer, 22% Carbon Black Filled
(discontinued **) Data provided by the manufacturer, Dyneon LLC.66% fluorine content. See the many specific grades of Fluorel™ fluoroelastomer in MatWeb. |
|||
Glass Transition Temp, Tg | -20.0 °C | -4.00 °F | ASTM D3417 |
REXtac Rextac® RT 2115 Amorphous Polyalphaolefin (APAO) Adhesive and Sealant Grade.Description: Propylene homopolymer and FDA compliantFeatures: High softening point and short open timeApplications: Component of hot melt adhesives, sealants and specialty.. |
|||
Glass Transition Temp, Tg | -20.0 °C | -4.00 °F | ASTM D3417 |
REXtac Rextac® RT 2180 Amorphous Polyalphaolefin (APAO) Adhesive and Sealant Grade.Description: Propylene homopolymer and FDA compliantFeatures: High softening point, short open time, good cohesive strength, and high viscosityApplications: Component of h.. |
|||
Glass Transition Temp, Tg | -20.0 °C | -4.00 °F | DMA |
Covestro Texin® DP7-3008 Thermoplastic Polyurethane, Polyester-based, Aliphatic
(discontinued **) Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This produ.. |
|||
Glass Transition Temp, Tg | -20.0 °C | -4.00 °F | |
Dow Pellethane® 2102-90AR Polyurethane Elastomer, Polyester Polycaprolactone Based
(discontinued **) PELLETHANE® 2102-90AR elastomer is a polyester polycaprolactone based polyurethane elastomer which combines excellent resistance to fuels and oils with enhanced mold release, low compression set, a.. |
|||
Glass Transition Temp, Tg | -20.0 °C | -4.00 °F | |
Mallard Creek Polymers Rovene® 6016 Acrylic Emulsion Applications: Rovene® 6016 is recommended for various nonwoven and paper applications requiring soft hand with resistance to heat and light aging coupled with good wet strength and chemical resis.. |
|||
Glass Transition Temp, Tg | -20.0 °C | -4.00 °F | ASTM D1329 |
Seals Eastern 5722 Fluorocarbon-Elastomer Formulated Viton®. General service.Information provided by Seals Eastern, Inc. |
|||
Glass Transition Temp, Tg | -20.0 °C | -4.00 °F | ASTM D1329 |
Seals Eastern 5722A Fluorocarbon-Elastomer Seals Eastern's formulated Viton® elastomers can be utilized in seals, o-rings, gaskets, packings and other applications where thermal stability and chemical resistance are required.Features:Exce.. |
|||
Glass Transition Temp, Tg | -20.0 °C | -4.00 °F | ASTM D1329 |
Seals Eastern 5723 Fluorocarbon-Elastomer Formulated Viton®. General service.Information provided by Seals Eastern, Inc. |
|||
Glass Transition Temp, Tg | -20.0 °C | -4.00 °F | ASTM D1329 |
Seals Eastern 5724 Fluorocarbon-Elastomer Formulated Viton®. General service.Information provided by Seals Eastern, Inc. |
|||
Glass Transition Temp, Tg | -20.0 °C | -4.00 °F | ASTM D1329 |
Seals Eastern 5725 Fluorocarbon-Elastomer Formulated Viton®. General service.Information provided by Seals Eastern, Inc. |
|||
Glass Transition Temp, Tg | -20.0 °C | -4.00 °F | ASTM D1329 |
Seals Eastern 5753 Fluorocarbon-Elastomer Features:MIL-SpecFKM general serviceInformation provided by Seals Eastern. |
|||
Glass Transition Temp, Tg | -20.0 °C | -4.00 °F | ASTM D1329 |
Seals Eastern 7130 Fluorocarbon-Elastomer FKM specially for oil & gas service.Information provided by Seals Eastern, Inc. |
|||
Glass Transition Temp, Tg | -20.0 °C | -4.00 °F | ASTM D1329 |
Seals Eastern 7148 Fluorocarbon-Elastomer FKM specially for oil & gas service; ED resistantInformation provided by Seals Eastern, Inc. |
|||
Glass Transition Temp, Tg | -20.0 °C | -4.00 °F | ASTM E1356 |
SK Chemicals SKYTHANE® US518 Adhesive (Dry Lamination) Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
Glass Transition Temp, Tg | -20.0 °C | -4.00 °F | ASTM D1329 |
Seals Eastern 7042 Fluorocarbon-Elastomer Seals Eastern's formulated Viton® elastomers can be utilized in seals, o-rings, gaskets, packings and other applications where thermal stability and chemical resistance are required.Features:Type.. |
|||
Glass Transition Temp, Tg | -20.0 °C | -4.00 °F | ASTM D4065 |
SK Chemicals SKYTHANE® 420 Hotmelt Grade UB Polyurethane SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr.. |
|||
Glass Transition Temp, Tg | -20.0 °C | -4.00 °F | ASTM D4065 |
SK Chemicals SKYTHANE® UB420 Hotmelt Lamination Film Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. UB series are used for adhesives and coating applications such as binder for magnetic ta.. |
|||
Glass Transition Temp, Tg | -20.0 °C | -4.00 °F | |
Unitika elitel UE3400 Polyester, Flake Elastomer, Rubber elasticity, Wide compatibility, Low temperature flexibilityUNITIKA l resins are thermoplastic saturated copolymeric polyester resins. l resins are expanding their applications fro.. |
|||
Glass Transition Temp, Tg | -20.0 °C | -4.00 °F | DSC |
Wolf Kunststoff ZEDEX® ZX-550 A5L Polymer Alloy Main Characteristics: Strong anti-adhesive; Low creep; Weather resistant; No water absorption; Good machinability; Strongly viscoelastic; Stress resistantApplications: Chemical Engineering; Laborato.. |
|||
Glass Transition Temp, Tg | -20.0 °C | -4.00 °F | DSC |
Wolf Kunststoff ZEDEX® ZX-550PV A7A Polymer Alloy Main Characteristics: Modified friction wear; Tough; Soft; Reduced wear at temperatures at 100 ° CApplications: Chemical Engineering; Laboratory Technology; Automitve Technology; Machine ToolsInfor.. |
|||
Glass Transition Temp, Tg | -20.0 °C | -4.00 °F | |
Dow Latex LXC 8429NA Carboxylated Styrene-Butadiene Latex Applications: Latex LXC 8429NA for carpet is a soft hand latex and is used in applications where a soft carpet hand is desired. These applications include some commercial and residential carpets, ru.. |
|||
Glass Transition Temp, Tg | -20.0 °C | -4.00 °F | 10°C/min |
Covestro Texin® 250 Urethane Thermoplastic Elastomer Key Features:UnfilledSuitable processing methods:Injection moldingProfile extrusionSheet extrusionCoatingBlow moldingInformation provided by Bayer Polymers.As of 1 September 2015, Bayer MaterialScie.. |
|||
Glass Transition Temp, Tg | -20.0 °C | -4.00 °F | Cured property; ASTM E831-86 |
Aptek UVISTAKE 7206 UV Curing, Urethane staking compound UVISTAKE 7206 is a 100% solid, thixotropic, one component, premixed frozen, electrically insulating, urethane system designed for the attachment and staking of electrical/electronic components mount.. |
|||
Glass Transition Temp, Tg | -20.0 °C | -4.00 °F | |
Loctite® Durabond® U-10FL Urethane Adhesive Urethane AdhesivesLoctite offers a complete line of one-part and two-part epoxy and urethane adhesives for structural bonding, potting and encapsulating. The Loctite® Durabond® line contains 14 ap.. |
|||
Glass Transition Temp, Tg | -20.0 °C | -4.00 °F | |
Lubrizol ESTANE® 58277 Ester Based Thermoplastic Polyurethane Features: Excellent physical properties, good chemical resistance and wide processing window for extrusion.Uses: Blown and flat die/cast film extrusion and Injection and blow molding.Complies with: .. |
|||
Glass Transition Temp, Tg | -20.0 °C | -4.00 °F | ASTM D1329 |
Seals Eastern 5717 Fluorocarbon-Elastomer FKM. General service.Information provided by Seals Eastern, Inc. |