Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 300000 ohm-cm | 300000 ohm-cm | |
Shakespeare Resistat® F901 N022 Nylon 6 Monofilament Resistat F901, MERGE N022 is a 22-denier nylon 6 monofilament which has electrically conductive carbon suffused into the surface. The filament has a round cross section with a coating thickness of .. |
|||
Electrical Resistivity | 300000 ohm-cm | 300000 ohm-cm | |
Shakespeare Resistat® F901 S022 Nylon 6 Monofilament Resistat F901, MERGE S022 is a 33-denier nylon 6 monofilament which has electrically conductive carbon suffused into the surface. The filament has a round cross section with a coating thickness of .. |
|||
Electrical Resistivity | 300000 ohm-cm | 300000 ohm-cm | |
Shakespeare Resistat® F9122 A400 Nylon 6 Monofilament Resistat F9122, MERGE A400 is a 22 denier per filament, 4 inch, conductive nylon 6 stable. Each filament has electrically conductive carbon suffused into the surface. The filaments have a round cr.. |
|||
Electrical Resistivity | 300000 ohm-cm @Temperature 1000 °C |
300000 ohm-cm @Temperature 1830 °F |
ASTM D1829 |
CoorsTek Mullite, S2 Thermal Shock Delta Tc = 300°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar.. |