Sharadaa Ceramics LI SILL-II High Alumina Brick

Category Ceramic , Oxide , Aluminum Oxide
Manufacturer Sharadaa Ceramics
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Sharadaa Ceramics LI SILL-II High Alumina Brick.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Services Offered: Retrofitting of Furnace, Installation of Castables/Bricks/Ceramic Fiber Modules, Castable Laying by Vibrocasting/Guiniting, Turnkey Installation Boiler/Chimney/Heater/Reformer/Rotary Kiln, Heat Curing and Acid Proof Lining Industry Focuses: Steel, Sponge, Rolling Mills, Coke Oven, Ferrous Foundries, Non-Ferrous, Cement, Petro Chemical, Mineral Processing, Sugar / Paper Mills and Chemical PlantsInformation provided by Sharadaa Ceramics Pvt. Ltd.
Physical Properties Metric English Comments
Bulk Density 2.35 g/cc
0.0849 lb/in³
Porosity 16 - 18 %
16 - 18 %
Mechanical Properties Metric English Comments
Compressive Strength 44.1 MPa
6400 psi
Cold Crushing
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 1500 °C
2730 °F
Component Elements Properties Metric English Comments
Al2O3 56 - 58 %
56 - 58 %
Fe2O3 1.0 - 1.2 %
1.0 - 1.2 %
Descriptive Properties Value Comments
PCE Orton 36
Permanent Linear Change -0.5 - 0.5%
1500°C