Physical Properties Metric English Comments
Bulk Density 2.35 - 2.45 g/cc
0.0849 - 0.0885 lb/in³
After drying at 110°C
Gouda Vuurvast CURON 150 GM Dense Refractory Castable
Description: Curon 150 GM is a gunmix based on sintered bauxite with an excellent thermal shock resistance and is therefore very well suited for burner blocks.Remarks: These values apply to cast pro..
Bulk Density 2.35 - 2.45 g/cc
0.0849 - 0.0885 lb/in³
After drying at 110°C
Gouda Vuurvast CURON 160 HS Dense Refractory Castable
Description: Because of the selection of raw materials, this castable has a high volume stability and a high strength up to high temperatures. In addition, Curon 160 HS has an excellent thermal shoc..
Bulk Density 2.35 g/cc
0.0849 lb/in³
Sharadaa Ceramics LI SILL-II High Alumina Brick
Services Offered: Retrofitting of Furnace, Installation of Castables/Bricks/Ceramic Fiber Modules, Castable Laying by Vibrocasting/Guiniting, Turnkey Installation Boiler/Chimney/Heater/Reformer/Rota..
Bulk Density >= 2.35 g/cc
>= 0.0849 lb/in³
Dried at 110°C
Sharadaa Ceramics REFCAST LC60ABR Low Cement Castables
Description: We bring to our clients a range of Low Cement Castables, that are available in varied alumina content and service range. Designed for abrasion resistance application, these are widely u..
Bulk Density 2.35 g/cc
0.0849 lb/in³
After Drying at 110°C
Sharadaa Ceramics Smart Cast 9 Medium Cement Castables
Information provided by Sharadaa Ceramics Pvt. Ltd.
Bulk Density 2.35 g/cc
0.0849 lb/in³
Chosun Refractories COD-1 Special brick
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Bulk Density 2.35 g/cc
0.0849 lb/in³
Chosun Refractories MSC-1 Blast Furnace Tap-Hole Refractory
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Bulk Density 2.35 g/cc
0.0849 lb/in³
Chosun Refractories PCB-50 Casting Block
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).