Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 120 MPa @Strain 5 % |
17400 psi @Strain 5 % |
ISO 604 |
Quadrant EPP Ketron® HPV PEEK + carbon fibres + PTFE + graphite, bearing grade, extruded (ISO Data) The addition of carbon fibres, PTFE and graphite to virgin PEEK results in a Ketron PEEK “bearing grade”. Its excellent tribological properties (low friction, long wear and high pressure-velocity .. |
|||
Compressive Strength | 120 MPa @Strain 5 % |
17400 psi @Strain 5 % |
ISO 604 |
Quadrant EPP Ketron® TX PEEK + solid lubricant, extruded (ISO Data) This member of the Ketron PEEK family has been developed especially for the food industry. Like Ketron PEEK-1000, this new internally lubricated material has a food contact compliant composition, bu.. |
|||
Compressive Strength | 120 MPa @Temperature 23.0 °C |
17400 psi @Temperature 73.4 °F |
Result based on 450G; ISO 604 |
Victrex® PEEK 600G Polyetheretherketone
(discontinued **) Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection moulding and extrusion, low viscosity, FDA food conta.. |
|||
Compressive Strength | 120 MPa @Temperature 200 °C |
17400 psi @Temperature 392 °F |
ISO 604 |
Victrex® PEEK 90HMF40 Polyetheretherketone (PEEK), 40% Carbon Fiber Reinforced Product Description: High performance thermoplastic material, 40% carbon fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding, easy flow, color black.Typica.. |
|||
Compressive Strength | 120 MPa @Temperature 23.0 °C |
17400 psi @Temperature 73.4 °F |
JIS K7208 |
Mitsui AURUM® 450 Thermoplastic Polyimide Resin, Non-filled
(discontinued **) AURUM® is an easy melt, processable and recyclable thermoplastic polyimide resin that provides continuous service temperatures to 465° F in its amorphous state and up to 550° F when annealed to i.. |
|||
Compressive Strength | 120 - 140 MPa @Temperature 1600 °C |
17400 - 20300 psi @Temperature 2910 °F |
Cold Crushing Strength |
Gouda Vuurvast CURAS 90 PF Moldable Refractory Material Description: Curas 90 PF ramming mix with outstanding abrasion properties, (erosion loss acc. ASTM C704: 2-4 cm3). The product is supplied in two components: a dry powder and a liquid. Curas 90 PF i.. |
|||
Compressive Strength | 120 - 140 MPa @Temperature 1600 °C |
17400 - 20300 psi @Temperature 2910 °F |
Cold Crushing Strength |
Gouda Vuurvast CURAS 90 PFM Moldable Refractory Material Description: Curas 90 PFM ramming mix has outstanding abrasion properties, (erosion loss acc. ASTM C704: 2-4 cm3). In addition, it has a good resistance against thermal shock and corrosive gasses. T.. |
|||
Compressive Strength | 120 MPa @Temperature 110 °C |
17400 psi @Temperature 230 °F |
Cold Crushing |
Sharadaa Ceramics VELECRETE RC 104 Rodding Castables Description: The Rodding Castables offered by us are user friendly in nature and does not require high energy mixing machines and vibrators. Free flowing in nature, these castables are designed in c.. |
|||
Compressive Strength | 120 MPa @Temperature 1400 °C |
17400 psi @Temperature 2550 °F |
Cold Crushing |
Sharadaa Ceramics VELECRETE RC 104 Rodding Castables Description: The Rodding Castables offered by us are user friendly in nature and does not require high energy mixing machines and vibrators. Free flowing in nature, these castables are designed in c.. |
|||
Compressive Strength | 120 MPa @Temperature 110 °C |
17400 psi @Temperature 230 °F |
Cold Crushing |
Sharadaa Ceramics VELECRETE RC 108 Rodding Castables Description: The Rodding Castables offered by us are user friendly in nature and does not require high energy mixing machines and vibrators. Free flowing in nature, these castables are designed in c.. |
|||
Compressive Strength | 120 MPa @Temperature 1400 °C |
17400 psi @Temperature 2550 °F |
Cold Crushing |
Sharadaa Ceramics VELECRETE RC 108 Rodding Castables Description: The Rodding Castables offered by us are user friendly in nature and does not require high energy mixing machines and vibrators. Free flowing in nature, these castables are designed in c.. |
|||
Compressive Strength | 120 MPa @Temperature 200 °C |
17400 psi @Temperature 392 °F |
|
Elisto THERMOSTAR® 4000 Mold Insulation Material Insulation of clamping platesInformation provided by elisto |
|||
Compressive Strength | 120 MPa @Temperature 23.0 °C |
17400 psi @Temperature 73.4 °F |
ISO 604 |
Victrex® PEEK 650G Polyetheretherketone Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection moulding and extrusion, low viscosity, FDA food conta.. |
|||
Compressive Strength | 120 MPa @Temperature 120 °C |
17400 psi @Temperature 248 °F |
ISO 604 |
Victrex® PEEK 650GL30 30% Glass Fiber Filled, PolyEtherEtherKetone High performance thermoplastic material, 30% glass fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding and extrusion, low flow, color natural/beige.Typical.. |