Material Notes:
Special Properties: Thermal Shock Slag ResistanceIndustry: SteelApplication: Pig Iron Laddle Safety Layer, Sponge Iron Rotary Kiln BackupInformation provided by Sharadaa Ceramics Pvt. Ltd.
Physical Properties Metric English Comments
Bulk Density >= 2.30 g/cc
>= 0.0831 lb/in³
After Drying at 110°C
Grain Size <= 5000 µm
<= 5000 µm
Mechanical Properties Metric English Comments
Compressive Strength 34.3 MPa

@Temperature 110 °C
4980 psi

@Temperature 230 °F
Cold Crushing
78.5 MPa

@Temperature 1100 °C
11400 psi

@Temperature 2010 °F
Cold Crushing
88.3 MPa

@Temperature 1500 °C
12800 psi

@Temperature 2730 °F
Cold Crushing
14.7 MPa

@Time 86400 sec
2130 psi

@Time 24.0 hour
Cold Crushing
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 1550 °C
2820 °F
Descriptive Properties Value Comments
Refractoriness >1680°C
Thermal Expansion 0.6
@ 1000°C, Reversible
Water Required to Mix 5-5.5%
Users viewing this material also viewed the following: