Material Notes:
Information Provided by Shin-Etsu Silicones of America, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.02 g/cc
1.02 g/cc
Viscosity 1000 cP
1000 cP
Mechanical Properties Metric English Comments
Hardness, Shore A 25
25
Tensile Strength at Break 1.50 MPa
218 psi
Thermal Properties Metric English Comments
Thermal Conductivity 0.150 W/m-K
1.04 BTU-in/hr-ft²-°F
Electrical Properties Metric English Comments
Dielectric Strength 24.0 kV/mm
610 kV/in
Dissipation Factor 0.00070

@Frequency 50.0 Hz
0.00070

@Frequency 50.0 Hz
Processing Properties Metric English Comments
Cure Time 60.0 min

@Temperature 100 °C
1.00 hour

@Temperature 212 °F
Descriptive Properties Value Comments
Colors Clear
Mix Ratio By Weight 1:01