Material Notes:
Information Provided by Shin-Etsu Silicones of America, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.07 g/cc
1.07 g/cc
Viscosity 75000 cP
75000 cP
Mechanical Properties Metric English Comments
Hardness, Shore A 40
40
Tensile Strength at Break 5.86 MPa
850 psi
Tear Strength 21.9 kN/m
125 pli
Processing Properties Metric English Comments
Cure Time 1440 min

@Temperature 23.0 °C
24.0 hour

@Temperature 73.4 °F
Descriptive Properties Value Comments
Colors Translucent
Mix Ratio By Weight 10:01