Polymer Property : Viscosity = 75000 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity 75000 cP

@Shear Rate 400 1/s,
Temperature 200 °C
75000 cP

@Shear Rate 400 1/s,
Temperature 392 °F
Premix Thermoplastics PRESEAL® TPE 6080
General Description:PRESEAL® TPE 6080 is a thermoplastic elastomer based highly conductive compound intended primarily for EMI gasket applications. It can also be used as conductors or in grounding..
Viscosity 75000 cP
75000 cP
Shin-Etsu Silicones KE-3479 Silicone, RTV
Information Provided by Shin-Etsu Silicones of America, Inc.
Viscosity 75000 cP
75000 cP
Shin-Etsu Silicones KE-1300T Silicone, Mold Making RTV
Information Provided by Shin-Etsu Silicones of America, Inc.
Viscosity 75000 cP
75000 cP
Shin-Etsu Silicones KE-1310ST Silicone, Mold Making RTV
Information Provided by Shin-Etsu Silicones of America, Inc.
Viscosity 75000 cP

@Temperature 25.0 °C
75000 cP

@Temperature 77.0 °F
Dynamic
Struktol POLYDIS 3693 Elastomer modified epoxy prepolymer
Applications: STRUKTOL POLYDIS 3693 is used as a tackyfier where conventional epoxy systems are unable to satisfy the demands of for example contact adhesion or peel strength. Improvements in the im..
Viscosity 75000 cP
75000 cP
Mixed - medium; Resin - 75,000 cP; Hardener - 65,500 cP
Loctite® Durabond® E-40FL Epoxy Adhesive
Epoxy AdhesivesLoctite offers a complete line of one-part and two-part epoxy and urethane adhesives for structural bonding, potting and encapsulating. The Loctite® Durabond® line contains 14 appli..
Viscosity 75000 cP
75000 cP
Dymax 9-20515 Peelable Mask
High Performance Light-Curing Adhesives and Coatings for Electronic AssemblyDymax 9-20515 Peelable MaskRed, non-slumping, non-stringing Cure Type: UV or Visible
Viscosity 75000 cP
75000 cP
Base
ACC QM 270 QSI Quantum Silicones 70 Durometer Addition Cure Moldmaking Material
QM 270 is a two component, room temperature addition cure silicone material. The cured rubber has excellent mechanical properties, good shelf-life stability, excellent physical properties and resin ..
Viscosity 75000 cP
75000 cP
Mixed Viscosity
Aremco Aremco-Bond™ 807 High Performance Epoxide
10 Minute Set, Non-Sagging, 1:1, Excellent Electrical & Mechanical Properties