Material Notes:
Excellent flame retardancy, good impact strength, good chemical resistance, good wear and abrasion resistance.Data provided by the manufacturer.
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
ASTM D792
Melt Flow 1.2 g/10 min
1.2 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 105
105
ASTM D785
Tensile Strength, Yield 45.0 MPa
6530 psi
ASTM D638
Izod Impact, Notched 2.14 J/cm
4.01 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 93.0 µm/m-°C

@Temperature 20.0 °C
51.7 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Flammability, UL94 V-0

@Thickness 2.54 mm
V-0

@Thickness 0.100 in
Electrical Properties Metric English Comments
Comparative Tracking Index 250 V
250 V
UL 746A
Hot Wire Ignition, HWI 33.4 sec
33.4 sec
UL746A
High Amp Arc Ignition, HAI 199.4 arcs
199.4 arcs
UL746A
High Voltage Arc-Tracking Rate, HVTR 149.0 mm/min
5.866 in/min
UL746A
Processing Properties Metric English Comments
Processing Temperature 177 - 216 °C
351 - 421 °F
Extrusion
204 - 227 °C
399 - 441 °F
Injection
Users viewing this material also viewed the following: