Material Notes:
Shall correspond to control sample, approved in accordance with the established procedure. Pores, which can be seen by eyes, are not allowed. Plastic shall no burn at stop of worm extruder for a period of 20 minutes. For molding of non-detachable plugs, connecting cords of electric machines and devices and for sheath of electric domestic cords. Characteristic peculiarity of plastic "Neva" is absence of sticking, changing of color of plastic during contact with metal surfaces, heated up to 150°C during 8-10 minutes.
Physical Properties Metric English Comments
Density 1.32 g/cc
0.0477 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength at Break >= 17.0 MPa
>= 2470 psi
Elongation at Break >= 250 %
>= 250 %
Thermal Properties Metric English Comments
Brittleness Temperature <= -35.0 °C
<= -31.0 °F
Electrical Properties Metric English Comments
Volume Resistivity >= 5.00e+12 ohm-cm

@Temperature 70.0 °C
>= 5.00e+12 ohm-cm

@Temperature 158 °F
Dielectric Strength >= 20.0 kV/mm
>= 508 kV/in
Descriptive Properties Value Comments
Color White