Material Notes:
For production of paints.
Physical Properties Metric English Comments
Solubility in Water >= 99 %
>= 99 %
Descriptive Properties Value Comments
Appearance Powder of porous crumb
Mass Share of Chlorine 61-64%
Mass Share of Iron <0.05%
Mass Share of Water <0.5%