Silberline Extra Fine "A"

Category Other Engineering Material , Additive/Filler for Polymer
Manufacturer Silberline
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Silberline Extra Fine "A".pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Extra Fine "A" is a standard polished grade; class "A", fine leafing aluminum pigment carried in mineral spirits.Applications: Trade & Maintenance
Physical Properties Metric English Comments
Specific Gravity 1.47 g/cc
1.47 g/cc
Bulk Factor 0.082
0.082
Volatiles 35 %
35 %
Particle Size 12 µm
12 µm
Particle Mesh Size <= 325 Mesh
<= 325 Mesh
0.1% retained
Descriptive Properties Value Comments
% Leaf (min) 55
Solvents Mineral Spirits
Water Coverage (cm²/gm) 32000