Material Notes:
SparkleBriteâ„¢ pigments are non-leafing aluminum pigment pastes carried in isopropyl alcohol. These grades are based on cornflake geometry and produce strong metallic effects in solvent and waterborne flexographic and gravure inks. Although SparkleBriteâ„¢ pigments can be used in aqueous inks they are not treated to protect against the aluminum-water reaction and special care must be taken to evaluate the gassing stability of each grade in the final ink formulation. High or excessive shear during ink production can initiate the aluminum-water reaction. Care must be taken to avoid excessive or high shear during processing when used in ink formulations containing water.Applications: Printing Inks
Physical Properties Metric English Comments
Specific Gravity 1.46 g/cc
1.46 g/cc
Volatiles 35 %
35 %
Particle Size 12 µm
12 µm
Descriptive Properties Value Comments
Category Non-leafing
Solvents Isopropyl Alcohol