Skamol Group SICAL 78 Silicon Nitride-Bonded Silicon Carbide Brick

Category Ceramic , Carbide
Manufacturer Skamol Group
Trade Name SICAL
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Skamol Group SICAL 78 Silicon Nitride-Bonded Silicon Carbide Brick.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Silicon nitride-bonded silicon carbide brick has the following characteristics: Max. service temperature 1580°C (2876°F)For sidewall lining of aluminum reduction cellsHigh thermal conductivityLow porosityLow thermal expansionLow gas permeabilityOutstanding abrasion and erosion resistanceHigh modulus of ruptureSuperior resistance to metal penetration and attackExtremely high crushing strengthExcellent oxidation resistance and resistance to corrosionInformation provided by Skamol.
Physical Properties Metric English Comments
Bulk Density 2.64 g/cc
0.0955 lb/in³
EN 993-1 1995
Porosity 17 %
17 %
Apparent; EN 993-1 1995
Permeability <= 0.050
<= 0.050
nPm, Permeability to gases; EN 993-4 1995
Mechanical Properties Metric English Comments
Modulus of Rupture 0.0440 GPa
6.38 ksi
EN 993-6: 1995
Compressive Strength 160 MPa
23200 psi
EN 993-5 1998
Thermal Properties Metric English Comments
CTE, linear 4.30 µm/m-°C

@Temperature 20.0 - 1000 °C
2.39 µin/in-°F

@Temperature 68.0 - 1830 °F
ASTM C-372
Thermal Conductivity 21.0 W/m-K

@Temperature 700 °C
146 BTU-in/hr-ft²-°F

@Temperature 1290 °F
Hot strip, Mean temp.; SINTEF
28.0 W/m-K

@Temperature 500 °C
194 BTU-in/hr-ft²-°F

@Temperature 932 °F
Hot strip, Mean temp.; SINTEF
38.0 W/m-K

@Temperature 200 °C
264 BTU-in/hr-ft²-°F

@Temperature 392 °F
Hot strip, Mean temp.; SINTEF
Maximum Service Temperature, Air 1580 °C
2880 °F
Component Elements Properties Metric English Comments
Al2O3 + Fe2O3 + CaO 0.50 %
0.50 %
Si3N4 18 %
18 %
SiC 78 %
78 %
Silicon, Si 0.50 %
0.50 %
SiO2 + Si2ON2 2.0 %
2.0 %
Descriptive Properties Value Comments
Color Grey
Corrosion Resistance 3
SINTEF
Dimensional Tolerances (Length/Width/Thickness) ±2.0/±2.0/±1.0 mm
Standard Sizes 510x300x50mm, 500x300x100mm, or 230x114x64mm
Other sizes made on request