Thermal Properties Metric English Comments
Thermal Conductivity 38.0 W/m-K

@Temperature 350 °C
264 BTU-in/hr-ft²-°F

@Temperature 662 °F
Latrobe LSSâ„¢ 2714 Hot Work Tool Steel (DIN 1.2714 mod)
TLS 2714 is a nickel-chromium-molybdenum hot work steel that exhibits high impact toughness and good resistance to softening at elevated temperature. The high nickel content imparts the toughness as..
Thermal Conductivity 38.0 W/m-K

@Temperature 350 °C
264 BTU-in/hr-ft²-°F

@Temperature 662 °F
Latrobe LSSâ„¢ 2714T Hot Work Tool Steel (DIN 1.2714 mod)
TLS 2714HT is the same steel available from inventory in a heat-treated condition, at a hardness of 352 to 401 HBS (approximately 38 to 43 HRC). TLS 2714HT can be readily flame cut, and this propert..
Thermal Conductivity 38.0 W/m-K

@Temperature 200 °C
264 BTU-in/hr-ft²-°F

@Temperature 392 °F
Hot strip, Mean temp.; SINTEF
Skamol Group SICAL 78 Silicon Nitride-Bonded Silicon Carbide Brick
Silicon nitride-bonded silicon carbide brick has the following characteristics: Max. service temperature 1580°C (2876°F)For sidewall lining of aluminum reduction cellsHigh thermal conductivity..
Thermal Conductivity 38.0 W/m-K

@Temperature 871 °C
264 BTU-in/hr-ft²-°F

@Temperature 1600 °F
ATI Wah Chang Nb/Nb Alloy C-103
This alloy satisfies most rocket engine applications for temperatures up to 2700°F because of superior mechanical properties at all temperatures. Offers weight savings over many rocket engine desig..