Material Notes:
SKAMOLEX panel designs have the following characteristics: Max. service temperature: Up to 1150°C (2102°F)Hot-face applications or back-up insulationA large variety of specialized and versatile highly insulating refractory panels and shapes made of vermiculiteResistant to high temperatures, withstand direct flame impingementGood electrical resistivityCustomized designs: Special shapes or panels, surface pattern and two-dimensional effectsAvailable in various combinations of bulk density, insulation properties and compressive strengthHave a myriad of uses and are ideally suited for lining hearth and heating appliances such as fireplaces, gasfires and stoves as well as night storage heaters, domestic boilers, and cooking appliancesAlso used in high temperature industries where special designs are required, possibly in combination with calcium silicate slabs.Information provided by Skamol.
Physical Properties Metric English Comments
Bulk Density 0.702 g/cc
0.0253 lb/in³
Dry
Loss On Ignition 6.00 %

@Temperature 1025 °C
6.00 %

@Temperature 1877 °F
Porosity 74 %
74 %
Total
Mechanical Properties Metric English Comments
Modulus of Rupture 0.00200 GPa
0.290 ksi
EN 993-6: 1995
Compressive Strength 4.50 MPa
653 psi
EN 1094-5: 1995
Thermal Properties Metric English Comments
CTE, linear 11.0 µm/m-°C

@Temperature 20.0 - 750 °C
6.11 µin/in-°F

@Temperature 68.0 - 1380 °F
BS 1902: section 5.3: 1990
Specific Heat Capacity 0.940 J/g-°C
0.225 BTU/lb-°F
Thermal Conductivity 0.180 W/m-K

@Temperature 200 °C
1.25 BTU-in/hr-ft²-°F

@Temperature 392 °F
Mean temp.; ASTM C-182
0.190 W/m-K

@Temperature 400 °C
1.32 BTU-in/hr-ft²-°F

@Temperature 752 °F
ASTM C-182
0.260 W/m-K

@Temperature 600 °C
1.80 BTU-in/hr-ft²-°F

@Temperature 1110 °F
ASTM C-182
Maximum Service Temperature, Air 1100 °C
2010 °F
Shrinkage 1.10 %

@Temperature 1000 °C,
Time 43200 sec
1.10 %

@Temperature 1830 °F,
Time 12.0 hour
Linear Reheat Shrinkage; EN 1094-6: 1999
Component Elements Properties Metric English Comments
Al2O3 7.0 %
7.0 %
CaO 5.0 %
5.0 %
Fe2O3 6.5 %
6.5 %
K2O 10 %
10 %
MgO 20 %
20 %
Na2O 0.10 %
0.10 %
SiO2 47 %
47 %
TiO2 1.0 %
1.0 %
Descriptive Properties Value Comments
Color Light Brown
Pyrometric Cone Equivalent 1300°C
ASTM C24-89, ORTON cones
Resistance to Thermal Shock Min 10 cycles
EN 993-11: 1998, heating to 950°C (1742°F)