Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 0.940 J/g-°C | 0.225 BTU/lb-°F | |
Skamol Group SKAMOLEX V-1100 (475) Customized Shape SKAMOLEX customized shapes have the following characteristics: Max. service temperature: Up to 1150°C (2102°F)Hot-face applications or back-up insulationA large variety of specialized and vers.. |
|||
Specific Heat Capacity | 0.940 J/g-°C | 0.225 BTU/lb-°F | |
Skamol Group SKAMOLEX V-1100 (600) Customized Shape SKAMOLEX customized shapes have the following characteristics: Max. service temperature: Up to 1150°C (2102°F)Hot-face applications or back-up insulationA large variety of specialized and vers.. |
|||
Specific Heat Capacity | 0.940 J/g-°C | 0.225 BTU/lb-°F | |
Skamol Group SKAMOLEX V-1100 (700) Customized Shape SKAMOLEX customized shapes have the following characteristics: Max. service temperature: Up to 1150°C (2102°F)Hot-face applications or back-up insulationA large variety of specialized and vers.. |
|||
Specific Heat Capacity | 0.940 J/g-°C | 0.225 BTU/lb-°F | |
Skamol Group SKAMOLEX V-1100 (700) Panel Design SKAMOLEX panel designs have the following characteristics: Max. service temperature: Up to 1150°C (2102°F)Hot-face applications or back-up insulationA large variety of specialized and versatil.. |
|||
Specific Heat Capacity | 0.940 J/g-°C | 0.225 BTU/lb-°F | |
Skamol Group SKAMOLEX V-1100 (800) Customized Shape SKAMOLEX customized shapes have the following characteristics: Max. service temperature: Up to 1150°C (2102°F)Hot-face applications or back-up insulationA large variety of specialized and vers.. |
|||
Specific Heat Capacity | 0.940 J/g-°C | 0.225 BTU/lb-°F | |
Skamol Group V-1100 375 Vermiculite Insulating Slab SKAMOL V-1100 & VIP-12 vermiculite slabs have the following characteristics: Max. service temperature: Up to 1150°C (2102°F)Hot-face applications or back-up insulation of all refractory constr.. |
|||
Specific Heat Capacity | 0.940 J/g-°C | 0.225 BTU/lb-°F | |
Skamol Group V-1100 410 Vermiculite Insulating Slab SKAMOL V-1100 & VIP-12 vermiculite slabs have the following characteristics: Max. service temperature: Up to 1150°C (2102°F)Hot-face applications or back-up insulation of all refractory constr.. |
|||
Specific Heat Capacity | 0.940 J/g-°C | 0.225 BTU/lb-°F | |
Skamol Group V-1100 475 Vermiculite Insulating Slab SKAMOL V-1100 & VIP-12 vermiculite slabs have the following characteristics: Max. service temperature: Up to 1150°C (2102°F)Hot-face applications or back-up insulation of all refractory constr.. |
|||
Specific Heat Capacity | 0.940 J/g-°C | 0.225 BTU/lb-°F | |
Skamol Group V-1100 600 Vermiculite Insulating Slab SKAMOL V-1100 & VIP-12 vermiculite slabs have the following characteristics: Max. service temperature: Up to 1150°C (2102°F)Hot-face applications or back-up insulation of all refractory constr.. |
|||
Specific Heat Capacity | 0.940 J/g-°C | 0.225 BTU/lb-°F | |
Skamol Group V-LITE 375 Vermiculite Insulating Brick V-LITE vermiculite insulating bricks have the following characteristics: Max. service temperature 1100°C (2012°F)Hot-face applications and back-up insulationGood insulation valueHigh mechanica.. |
|||
Specific Heat Capacity | 0.940 J/g-°C | 0.225 BTU/lb-°F | |
Skamol Group V-LITE 475 Vermiculite Insulating Brick V-LITE vermiculite insulating bricks have the following characteristics: Max. service temperature 1100°C (2012°F)Hot-face applications and back-up insulationGood insulation valueHigh mechanica.. |