Solvay ALKAMULS® R 81 Surfactant

Category Fluid , Other Engineering Material , Additive/Filler for Polymer
Manufacturer Solvay
Trade Name ALKAMULS®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay ALKAMULS® R 81 Surfactant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Biodegradable castor oil ethoxylate emulsifier, solubiliser for a wide range of formulations with an HLB of around 9.Chemical Name: ETHOXYLATED CASTOR OILCAS: 61791 - 12 – 6Solubility: Dispersible in water. Soluble in most polar and aromatic solvents. Available in: Asia Pacific, Europe, Latin America and North AmericaApplications: Nonionic emulsifier for metal working and agrochemical formulations. Emulsifier for oil and waxes in water based formulations. Often used in textile lubricants, and in food contact formulations.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.02 g/cc
0.0368 lb/in³
pH 7.0 - 8.5
7.0 - 8.5
5% in water; RPG02
Thermal Properties Metric English Comments
Pour Point <= 0.000 °C
<= 32.0 °F
Flash Point >= 100 °C
>= 212 °F
Processing Properties Metric English Comments
Moisture Content <= 0.50 %
<= 0.50 %
RPG16
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Appearance Viscous Liquid
Composition Active
1
HLB number 9.2
Ionic Charge Nonionic
Saponification number 99-105 mg KOH/g
RPG05