Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.280 W/m-K | 1.94 BTU-in/hr-ft²-°F | |
Murtfeldt Murylon® A Nylon 66 This material combines the excellent properties of the Murylon® range with additional high tensile and compressive strength, increased wear resistance, and a lower level of moisture absorption than.. |
|||
Thermal Conductivity | 0.280 W/m-K | 1.94 BTU-in/hr-ft²-°F | DIN.52612 (dry sample) |
Omnia Plastica Akulon® PA6 G.Oil - Omniamid Oil - at 50% RH Cast Nylon 6 with the addition of 6% of special lubricating oil which remains in solution in the material. The unique method of production results in a micro distribution of oil particles with a hom.. |
|||
Thermal Conductivity | 0.280 W/m-K | 1.94 BTU-in/hr-ft²-°F | DIN.52612 |
Omnia Plastica Akulon® PA6 G.Oil Omniamid Oil - Dry Cast Nylon 6 with the addition of 6% of special lubricating oil which remains in solution in the material. The unique method of production results in a micro distribution of oil particles with a hom.. |
|||
Thermal Conductivity | 0.280 W/m-K | 1.94 BTU-in/hr-ft²-°F | DIN.52612 (dry sample) |
Omnia Plastica Omniamid PA6 G - G - at 50% RH Cast nylon 6. The method of production of this polyamide (i.e. the polymerisation of the caprolactam directly in the mould) allows the production of stock shapes in larger than normal dimensions, su.. |
|||
Thermal Conductivity | 0.280 W/m-K | 1.94 BTU-in/hr-ft²-°F | |
Quadrant EPP Nylatron® MD PA 6 + metal detectable additive, extruded (ISO Data) Metal detectable 6SA grade High wear and fatigue resistance Lower moisture absorption than standard PA6 Metal and visual detection by blue colour Detection by x-ray also possible Continuous use temp.. |
|||
Thermal Conductivity | 0.280 - 0.400 W/m-K | 1.94 - 2.78 BTU-in/hr-ft²-°F | Average value: 0.360 W/m-K Grade Count:3 |
Overview of materials for Nylon 66, Glass/Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass/Carbon Fiber Filled". Each property range of values reported is minimum and maximum valu.. |
|||
Thermal Conductivity | 0.280 W/m-K | 1.94 BTU-in/hr-ft²-°F | DOM 52612 |
Manifattura Cattaneo PA 6 Nylon Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a. |
|||
Thermal Conductivity | 0.280 W/m-K | 1.94 BTU-in/hr-ft²-°F | DOM 52612 |
Manifattura Cattaneo PA 6.6 Nylon Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a. |
|||
Thermal Conductivity | 0.280 W/m-K | 1.94 BTU-in/hr-ft²-°F | ISO 8301:1991 |
Global EPP PA 6E Extruded Polyamide 6 Polyamides, commonly referred to as nylons, are macromolecular, partially crystalline thermoplastics. Their physical properties are mainly determined by the composition and structure of their molecu.. |
|||
Thermal Conductivity | 0.280 W/m-K | 1.94 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics NORYL SE1GFN2 PPE+HIPS (Europe-Africa-Middle East) Noryl* SE1GFN2 is a 20% glass reinforced, injection moldable modified polyphenylene ether resin. Designed for improved dimensional stability and good flow , this resin also uses non-chlorinated, non.. |
|||
Thermal Conductivity | 0.280 W/m-K | 1.94 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics NORYL V01525 PPE+HIPS (Asia Pacific) Noryl* V01525 is a 15% milled fiber reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
Thermal Conductivity | 0.280 W/m-K | 1.94 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics NORYL V01550 PPE+HIPS (Europe-Africa-Middle East) NORYL V01550 is a 15 % short glass fibre reinforced, flame retardant material with a HDT/A of 130C according ISO 75. NORYL V01550 is V0 at 0.75 mm according UL94 and is halogen free according VDE/DI.. |
|||
Thermal Conductivity | 0.280 W/m-K | 1.94 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics NORYL V03505 PPE+HIPS (Europe-Africa-Middle East) Noryl* V03505 is a 35% milled fiber reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
Thermal Conductivity | 0.280 W/m-K | 1.94 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics ULTEM 2200 PEI (Europe-Africa-Middle East) 20% Glass fiber filled, standard flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 and 5VA listing. |
|||
Thermal Conductivity | 0.280 W/m-K | 1.94 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics Ultem 2200N PEI 20% Glass fiber filled Polyetherimide (Tg 217C). ECO Conforming.This data was supplied by SABIC-IP for the Americas region. |
|||
Thermal Conductivity | 0.280 W/m-K | 1.94 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics Ultem 2200N PEI (Asia Pacific) 20% Glass fiber filled Polyetherimide (Tg 217C). ECO Conforming.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Thermal Conductivity | 0.280 W/m-K | 1.94 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics ULTEM 2210 PEI (Europe-Africa-Middle East) 20% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 and 5VA listing. |
|||
Thermal Conductivity | 0.280 W/m-K | 1.94 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics ULTEM 2210F PEI (Europe-Africa-Middle East) 20% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). Resin is RoHS compliant. US FDA and European Food Contact approved. Effective June, 2007 this grade will no longer be supported with b.. |
|||
Thermal Conductivity | 0.280 W/m-K | 1.94 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics NORYL GFN3V PPE+HIPS (Europe-Africa-Middle East) NORYL GFN3V is a 30 % glass fibre reinforced material with a HDT/A of 145C according ISO 75. NORYL GFN3V has been approved for potable water applications up to 85C by the UK WFBS according BS 6920 i.. |
|||
Thermal Conductivity | 0.280 W/m-K | 1.94 BTU-in/hr-ft²-°F | DIN 52612 |
Zell-Metall Engineering Plastics Zellamid 1100 MO Improved sliding and self lubricating properties are achieved by the addition of molybdenum disulphide. UV-radiation resistance is enhanced.Color: blackApplications: For conveyor screws |
|||
Thermal Conductivity | 0.280 W/m-K | 1.94 BTU-in/hr-ft²-°F | DIN 52612 |
Zell-Metall Engineering Plastics Zellamid 1100 OIL at 50% RH Zellamid® 1100 OIL: A new type of cast nylon produced by addition of a special oil to the polymer structure. By laboratory test it was proven that this second generation oil filled product reduces .. |
|||
Thermal Conductivity | 0.280 - 0.360 W/m-K | 1.94 - 2.50 BTU-in/hr-ft²-°F | |
Arlon 0.008" (0.2032 mm) Thermabond® Uncured Silicone (99510N008) 0.008 in., ±0.001 (0.2 mm, ±0.03) uncured silicone on 0.003 in. (0.08 mm) nominal PTFE coated fiberglass; 0.001 in. (0.03 mm) FEP interleave; overall thickness 0.008 in ±0.001(0.2 mm ± 0.03). T.. |
|||
Thermal Conductivity | 0.280 W/m-K | 1.94 BTU-in/hr-ft²-°F | DIN 52612 |
BASF Ultramid® KR 4355 G7 35% Glass Filled PA6/6T (Dry) Description: 35% glass-fiber reinforced product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechanical properties r.. |
|||
Thermal Conductivity | 0.280 W/m-K | 1.94 BTU-in/hr-ft²-°F | DIN 52612 |
BASF Ultramid® KR 4355 G7 BK 00564 35% Glass Filled PA6/6T (Conditioned) Description: 35% glass-fiber reinforced product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechanical properties r.. |
|||
Thermal Conductivity | 0.280 W/m-K | 1.94 BTU-in/hr-ft²-°F | |
CENTROPLAST CENTROMID 6 E Polyamide 6 extruded This tough and impact resistant material has good chemical resistance and can be bonded and welded. It is used for sealing rings, flanges, etc. Information provided by CENTROPLAST Engineering Plast.. |
|||
Thermal Conductivity | 0.280 W/m-K | 1.94 BTU-in/hr-ft²-°F | |
CENTROPLAST CENTROMID 6.6 FG Polyamide 6.6, Food Grade This material has good hardness, wear resistance, abrasion strength and impact strength.Information provided by CENTROPLAST Engineering Plastics GMBH |
|||
Thermal Conductivity | 0.280 W/m-K | 1.94 BTU-in/hr-ft²-°F | ASTM C 177 |
Adamas Adalon® 463 PTFE, 15% Special Polyimide Information provided by Adamas, HPM |
|||
Thermal Conductivity | 0.280 W/m-K | 1.94 BTU-in/hr-ft²-°F | |
CENTROPLAST CENTROMID 6 E FG Polyamide 6 extruded, Food Grade This tough and impact resistant material has good chemical resistance and can be bonded and welded. Information provided by CENTROPLAST Engineering Plastics GMBH |
|||
Thermal Conductivity | 0.280 W/m-K | 1.94 BTU-in/hr-ft²-°F | |
CENTROPLAST CENTROMID 6.6 Polyamide 6.6 This material has good hardness, wear resistance, abrasion strength and impact strength. It is used for bearing cages, sliding bearings and articulated joint blocks.Information provided by CENTROPL.. |