Solvay MACKANATE® OPV-N Surfactant

Category Fluid
Manufacturer Solvay
Trade Name MACKANATE®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay MACKANATE® OPV-N Surfactant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: Mackanate OPV-N is a vegetable derived, amido type monoester sulfosuccinate. It is a high foaming surfactant, mild to both eyes and skin with thickening properties. Mackanate OPV-N can be formulated with a variety of different anionics to produce high foaming skin cleaners with reduced irritation potential to both skin and eyes. Mackanate OPV-N also responds readily to viscosity builders such as amides, betaines and salts, allowing high viscosity products to be easily formulated. This product has no formaldehyde donors and contains no parabens. INCI Name: Disodium Oleamido MIPA Sulfosuccinate CAS: 43154-85-4 EINECS: 256-120-0 Uses: Mild Shampoos, Baby Shampoos, Sulfate Free Formulations and Body WashInformation provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.11 g/cc
0.0401 lb/in³
Solids Content 36.5 - 39.5 %
36.5 - 39.5 %
Moisture Balance
pH 5.0 - 7.5
5.0 - 7.5
5% Solution
Viscosity <= 2000 cP
<= 2000 cP
#3 SP @ 12 rpm
Optical Properties Metric English Comments
Gardner Color Number <= 6.0
<= 6.0
Processing Properties Metric English Comments
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Appearance Clear Liquid
Composition Total Plate Count
<10 cfu/g
Preservative Methylisothiazolinone
95 ppm