Solvay Specialty Polymers Amodel® A-1565 HS Polyphthalamide (PPA), 65% GlassMineral (Conditioned)

Category Polymer , Thermoplastic , Polyphthalamide (PPA) , Polyphthalamide (PPA), Mineral Filled
Manufacturer Solvay Specialty Polymers
Trade Name Amodel®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers Amodel® A-1565 HS Polyphthalamide (PPA), 65% GlassMineral (Conditioned).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Amodel® A-1565 HS is a 65% glass and mineral-reinforced polyphthalamide (PPA) designed to be cost-effective in applications requiring high stiffness, good dimensional stability and good retention of stiffness at elevated temperatures. This grades also exhibits a high deflection temperature and flexural modulus.Features: Good Chemical Resistance; Good Creep Resistance; Good Dimensional Stability; High Heat Resistance; Low CLTE; Low Warpage; Lubricated; Ultra High StiffnessUses: Automotive Applications; Automotive Under the Hood; Housings; Industrial Applications; Industrial Parts; Pump PartsInjection Molding Notes: Amodel® compounds are shipped in moisture-resistant packages at moisture levels according to specifications. Sealed, undamaged bags should be preferably stored in a dry room at a maximum temperature of 50°C (122°F) and should be protected from possible damage. If only a portion of a package is used, the remaining material should be transferred into a sealable container. It is recommended that Amodel® resins be dried prior to molding.Automotive Specifications ASTM D4000 PA121 R65 Color: BK324 Black; ASTM D6779 PA121R65; DELPHI M-53294 Color: BK324 BlackInformation provided by Solvay Specialty Polymers.
Physical Properties Metric English Comments
Density 1.90 g/cc
0.0686 lb/in³
Dry; ISO 1183
Filler Content 65 %
65 %
GlassMineral
Linear Mold Shrinkage, Flow 0.0030 cm/cm
0.0030 in/in
Dry
Linear Mold Shrinkage, Transverse 0.0050 cm/cm
0.0050 in/in
Dry; ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength 123 MPa
17800 psi
ASTM D638
Elongation at Break 1.2 %
1.2 %
ASTM D638
Tensile Modulus 20.8 GPa
3020 ksi
ASTM D638
Flexural Strength 196 MPa
28400 psi
ASTM D790
Flexural Modulus 18.0 GPa
2610 ksi
ASTM D790
Shear Strength 49.6 MPa
7190 psi
ASTM D732
Izod Impact, Notched 0.320 J/cm
0.599 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 311 °C
592 °F
Peak; Dry; ASTM D3418
311 °C
592 °F
Dry; ISO 11357-3
Processing Properties Metric English Comments
Processing Temperature 79.4 °C
175 °F
Hopper
Rear Barrel Temperature 304 - 318 °C
579 - 604 °F
Front Barrel Temperature 316 - 329 °C
601 - 624 °F
Melt Temperature 321 - 343 °C
610 - 649 °F
Mold Temperature 135 °C
275 °F
Drying Temperature 120 °C

@Time 14400 sec
248 °F

@Time 4.00 hour
Moisture Content <= 0.045 %
<= 0.045 %
Descriptive Properties Value Comments
Additive Heat Stabilizer
Availability Africa & Middle East
Asia Pacific
Europe
Latin America
North America
Color Black
Form Pellets
Processing Technique Injection Molding
RoHS Compliance RoHS Compliant