Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay Specialty Polymers Amodel® AF-1145 V0 Polyphthalamide (PPA) Resin, 45% Glass Reinforced, at 50% RH  (di

Category Polymer , Thermoplastic , Polyphthalamide (PPA) , Polyphthalamide (PPA), 50% Glass Fiber Reinforced
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers Amodel® AF-1145 V0 Polyphthalamide (PPA) Resin, 45% Glass Reinforced, at 50% RH  (di.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
AMODEL AF-1145 V0 is a 45% glass reinforced, flame retarded polyphthalamide (PPA) which exhibits a high heat distortion temperature, high tensile strength and flexural modulus. The material is relatively insensitive to moisture which results in good dimensional stability. Therefore, typical humid environmental conditions result in only minor changes in the strength and stiffness. This grade of AMODEL resin can withstand the demanding vapor phase and infrared reflow soldering processes typically used in the electronics industry. It is ideally suited for connectors and electrical devices requiring surface mount technology (SMT). The material offers easy processing using conventional equipment and methods.This product line was acquired by Solvay Advanced Polymers from BP Amoco in November 2001.MatWeb has an entry for this material dry as molded.
Physical Properties Metric English Comments
Density 1.81 g/cc
0.0654 lb/in³
Dry As Molded
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 177 MPa
25700 psi
ASTM D638
Tensile Modulus 18.0 GPa
2610 ksi
ASTM D638
Flexural Yield Strength 243 MPa
35200 psi
ASTM D790
Flexural Modulus 18.0 GPa
2610 ksi
ASTM D790
Izod Impact, Notched 0.590 J/cm
1.11 ft-lb/in
ASTM D256
Processing Properties Metric English Comments
Melt Temperature 321 - 338 °C
610 - 640 °F
Injection