Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay Specialty Polymers Amodel® DW-1130 Polyphthalamide (PPA), 30% Glass Fiber

Category Polymer , Thermoplastic , Polyphthalamide (PPA) , Polyphthalamide (PPA), 30% Glass Fiber Reinforced
Manufacturer Solvay Specialty Polymers
Trade Name Amodel®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers Amodel® DW-1130 Polyphthalamide (PPA), 30% Glass Fiber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Amodel® DW-1130 is a 30% glass-fiber-reinforced resin designed for high strength and stiffness and improved hydrolytic stability. This material has low moisture absorption and a low coefficient of thermal expansion, which means excellent dimensional stability. Creep resistance is also exceptional.Features: Chlorine Resistant; Good Chemical Resistance; Good Creep Resistance; Good Dimensional Stability; Good Stiffness; Good Strength; High Temperature Strength; Low Moisture AbsorptionUses: Appliances; Consumer Applications; Filters; Housings; Industrial Applications; Plumbing Parts; Pump Parts; Valves/Valve PartsInjection Molding Notes: Amodel® compounds are shipped in moisture-resistant packages at moisture levels according to specifications. Sealed, undamaged bags should be preferably stored in a dry room at a maximum temperature of 50°C (122°F) and should be protected from possible damage. If only a portion of a package is used, the remaining material should be transferred into a sealable container. It is recommended that Amodel® resins be dried prior to molding.Additional Properties: Flexural Strain at Break - ISO 178 (23°C): 2.9 %Information provided by Solvay Specialty Polymers.
Physical Properties Metric English Comments
Density 1.45 g/cc
0.0524 lb/in³
ISO 1183
Filler Content 30 %
30 %
Glass Fiber
Mechanical Properties Metric English Comments
Tensile Strength at Break 210 MPa
30500 psi
ISO 527-2
Elongation at Break 2.3 %
2.3 %
ISO 527-2
Tensile Modulus 11.9 GPa
1730 ksi
ISO 527-2
Flexural Strength 300 MPa
43500 psi
ASTM D790
Flexural Modulus 11.0 GPa
1600 ksi
ISO 178
Izod Impact, Notched (ISO) 7.20 kJ/m²
3.43 ft-lb/in²
ISO 180
Charpy Impact Unnotched 5.60 J/cm²
26.6 ft-lb/in²
ISO 179
Charpy Impact, Notched 0.720 J/cm²
3.43 ft-lb/in²
ISO 179
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 290 °C
554 °F
Unannealed; Flatwise; ISO 75-2/A
Processing Properties Metric English Comments
Rear Barrel Temperature 315 - 330 °C
599 - 626 °F
Middle Barrel Temperature 320 - 340 °C
608 - 644 °F
Front Barrel Temperature 325 - 345 °C
617 - 653 °F
Melt Temperature 340 - 360 °C
644 - 680 °F
Mold Temperature 160 °C
320 °F
Drying Temperature 120 °C

@Time 14400 sec
248 °F

@Time 4.00 hour
Moisture Content 0.030 - 0.060 %
0.030 - 0.060 %
Suggested Max
Descriptive Properties Value Comments
Availability Africa & Middle East
Asia Pacific
Europe
Latin America
North America
Color Black; Natural
Form Pellets
Processing Technique Injection Molding
RoHS Compliance RoHS Compliant
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved