Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 330 - 360 °C | 626 - 680 °F | |
LATI LAPEX A G/10 10% Glass Fiber Reinforced Polyethersulfone (PES) (UL94 V-0)
(Unverified Data**) Description: Lapex A compounds are polyethersulfone (PES) products. They are high temperature compounds offering an interesting combination of properties. Lapex A provides outstanding thermal resist.. |
|||
Melt Temperature | 330 - 360 °C | 626 - 680 °F | |
LATI LAPEX A G/20 20% Glass Fiber Reinforced Polyethersulfone (PES) (UL94 V-0)
(Unverified Data**) Description: Lapex A compounds are polyethersulfone (PES) products. They are high temperature compounds offering an interesting combination of properties. Lapex A provides outstanding thermal resist.. |
|||
Melt Temperature | 330 - 360 °C | 626 - 680 °F | |
LATI LAPEX A G/30 30% Glass Fiber Reinforced Polyethersulfone (PES) (UL94 V-0)
(Unverified Data**) Description: Lapex A compounds are polyethersulfone (PES) products. They are high temperature compounds offering an interesting combination of properties. Lapex A provides outstanding thermal resist.. |
|||
Melt Temperature | 338 - 360 °C | 640 - 680 °F | Molding |
PolyOne Lubri-Tech™ PF-000/15T Polysulfone, PTFE Lubricated
(discontinued **) Description/Features:PTFE LubricatedUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Melt Temperature | 338 - 360 °C | 640 - 680 °F | Stock |
PolyOne Stat-Tech™ PF-05CF/000 EM FR Flame Retardant Polysulfone - 5% Carbon Fiber
(discontinued **) Data provided by PolyOne. |
|||
Melt Temperature | 320 - 360 °C | 608 - 680 °F | |
LATI LAXTAR G/30 30% Glass Reinforced LCP
(discontinued **) Description: Laxtar products are liquid crystal polymers (LCP). They offer exceptional performance together with increasing cost-effectiveness. Due to the outstanding fluidity at high shear rates LC.. |
|||
Melt Temperature | 310 - 360 °C | 590 - 680 °F | |
LG Chemical LUCON PO-5300H Electrically Conductive Thermoplastic LG Chemicals has formulated a diverse range of LUCON thermoplastic compounds containing conductive additives, such as carbon powder, (nickel coated) carbon fiber, or stainless steel fiber for solvin.. |
|||
Melt Temperature | 310 - 360 °C | 590 - 680 °F | |
LG Chemical LUCON PO-5300M Electrically Conductive Thermoplastic LG Chemicals has formulated a diverse range of LUCON thermoplastic compounds containing conductive additives, such as carbon powder, (nickel coated) carbon fiber, or stainless steel fiber for solvin.. |
|||
Melt Temperature | 340 - 360 °C | 644 - 680 °F | |
Solvay Specialty Polymers Amodel® DW-1130 Polyphthalamide (PPA), 30% Glass Fiber Amodel® DW-1130 is a 30% glass-fiber-reinforced resin designed for high strength and stiffness and improved hydrolytic stability. This material has low moisture absorption and a low coefficient o.. |
|||
Melt Temperature | 340 - 360 °C | 644 - 680 °F | |
Solvay Specialty Polymers Amodel® DW-1140 Polyphthalamide (PPA), 40% Glass Fiber Amodel® DW-1140 is a 40% glass-fiber-reinforced resin designed for high strength and stiffness and improved hydrolytic stability. This material has low moisture absorption and a low coefficient o.. |
|||
Melt Temperature | 340 - 360 °C | 644 - 680 °F | |
Solvay Specialty Polymers Amodel® FC -1160 Polyphthalamide (PPA), 60% Glass Fiber Amodel® FC-1160 is an FDA-approved, 60% glass fiber reinforced resin designed for high strength and stiffness. This combines with its excellent thermal properties, low water absorption and good h.. |
|||
Melt Temperature | 340 - 360 °C | 644 - 680 °F | |
Solvay Specialty Polymers Amodel® FC-1140 Polyphthalamide (PPA), 40% Glass Fiber Amodel® FC-1140 is an FDA-approved, 40% glass fiber reinforced resin designed for high strength and stiffness. This combines with its excellent thermal properties, low water absorption and good h.. |
|||
Melt Temperature | 340 - 360 °C | 644 - 680 °F | |
Solvay Specialty Polymers Amodel® FC-1150 Polyphthalamide (PPA), 50% Glass Fiber Amodel® FC-1150 is an FDA-approved, 50% glass fiber reinforced resin designed for high strength and stiffness. This combines with its excellent thermal properties, low water absorption and good h.. |
|||
Melt Temperature | 350 - 360 °C | 662 - 680 °F | |
E-Polymers SEPAZ® C230GP 30% Glass Fiber Reinforced LCP Resin Liquid Crystal Polymer Resin: SEPAZ LCP resin has a unique structure and performance unthought of in a traditional plastics. Beside SEPAZ LCP takes the excels in all-around performance and molding .. |
|||
Melt Temperature | 350 - 360 °C | 662 - 680 °F | |
E-Polymers SEPAZ® C130GP 30% Glass Fiber Reinforced LCP Resin Liquid Crystal Polymer Resin: SEPAZ LCP resin has a unique structure and performance unthought of in a traditional plastics. Beside SEPAZ LCP takes the excels in all-around performance and molding .. |
|||
Melt Temperature | 338 - 360 °C | 640 - 680 °F | Molding |
PolyOne Edgetek® PF-1000 Polysulfone
(discontinued **) The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Melt Temperature | 321 - 360 °C | 610 - 680 °F | |
Solvay Specialty Polymers Xydar® G-930 Liquid Crystal Polymer (LCP)
(Unverified Data**) Xydar G-930 Liquid Crystal Polymer (LCP) is a glass reinforced injection molding grade developed specifically for electrical/electronic applications utilizing surface mount technology. The moldabili.. |
|||
Melt Temperature | 350 - 360 °C | 662 - 680 °F | |
E-Polymers SEPAZ® C140GP 40% Glass Fiber Reinforced LCP Resin Liquid Crystal Polymer Resin: SEPAZ LCP resin has a unique structure and performance unthought of in a traditional plastics. Beside SEPAZ LCP takes the excels in all-around performance and molding .. |