Solvay Specialty Polymers Diofan® A 736 Polyvinylidene Chloride (PVDC)  (Unverified Data**)

Category Polymer , Thermoplastic , PVDC , Polyvinyl Dichloride (PVDC)
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers Diofan® A 736 Polyvinylidene Chloride (PVDC)  (Unverified Data**).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DIOFAN® A 736 is a PVDC latex used as a flexible underlayer for coating on paper, cardboard and rigid PVC foils, to be covered with an appropriate topcoat.Additional Information: PROCESSING - DRYING - DIOFAN® A 736 has a medium surface tension. It can be processed with different coating techniques, including reverse gravure roll and air knife coating systems. - A good quality coating requires adequate drying, since higher temperatures will result in better barrier properties. FOOD AND DRUG LEGISLATIONS - The monomers used for the production of DIOFAN® A 736 comply with the requirements of the EU Commission Regulation No 10/2011 of 14 January 2011. - All the components are listed in the European Resolution AP 2004 (Surface coating intended to come into contact with foodstuffs). - DIOFAN® A 736 complies with U.S. FDA chapters 21 CFR 176.170 and 176.180. - The drug master file number for DIOFAN® A 736 is 11383. - The monomers used for the production of DIOFAN® A 740 comply with the Regulation (EC) 1907/2006 of the European Parliament and of the Council of 18 december 2006 concerning the Registration, Evaluation, Authorization and Restriction of Chemicals (REACH). - SolVin will provide necessary certification upon request by its customers. ISO CERTIFICATION - The implemented management system for the production, internal transfer and delivery, design and development of DIOFAN vinylidene chloride copolymers (PVDC) produced in Tavaux has been assessed and found to meet the requirements of ISO 9001: 2008, ISO 14001: 2004 and OHSAS 18001: 2007.Information provided by Solvay Specialty Polymers.
Physical Properties Metric English Comments
Density 1.300 g/cc
0.04697 lb/in³
1.650 g/cc
0.05961 lb/in³
Coating; 40 g/m² PVDC coating on PVC 250
Solids Content 60 %
60 %
pH 2.5
2.5
Water Vapor Transmission 18.0 g/m²/day

@Temperature 38.0 °C
1.16 g/100 in²/day

@Temperature 100 °F
90% RH;1 µm Coating on PVC
Oxygen Transmission Rate 21.0 cc/m²/day
1.35 cc/100 in²/day
25°C, 1.0 µm, 85% RH; Coating on BOPP
Viscosity 20 cP

@Temperature 20.0 °C
20 cP

@Temperature 68.0 °F
Surface Tension 45 dynes/cm
45 dynes/cm
Foaming tendency
Mechanical Properties Metric English Comments
Tensile Impact Strength 500 kJ/m²
238 ft-lb/in²
Coating properties: 40 g/m² PVDC coating on PVC
Processing Properties Metric English Comments
Shelf Life 12.0 Month
12.0 Month
23°C
Descriptive Properties Value Comments
Agency Ratings EC 1907/2006 (REACH)
EU No 10/2011
FDA 21 CFR 176.170
FDA 21 CFR 176.180
Availability Asia Pacific
Europe
North America
Ball Drop Test > 900 mm
Emulsion Type Anionic
Features Good Flexibility
Filmability 17°C
Minimum Film Forming Temperature
Forms Liquid
Generic PVDC
Uses Coating Applications