Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 20 cP | 20 cP | |
Resin Technology Group 85 Metal Bonder Fusion™ Cyanoacrylate Instant Ethyl Adhesive Resin Technology Group 85 Metal Bonder Fusion™ Cyanoacrylate Instant Ethyl Adhesive |
|||
Viscosity | 20 - 60 cP | 20 - 60 cP | |
Huntsman HY 1341 Cycloaliphatic Amine Approx. H+ equivalent weight 115. Mix Ratio with GY 6010 is 60.Comments/Applications: Low viscosity, modified amine for fast cure, resistant to acids, alkali, solvents. Mortar and floor repair, s.. |
|||
Viscosity | 20 - 80 cP | 20 - 80 cP | |
Huntsman Kerimid 701-1 B US Resin Comments/Applications: Used with Kerimid 701 A US for high Tg laminate systems. Suggested ratio 3 parts A to 1 part B.Data provided by Ciba Specialty Chemicals.Ciba Specialty Chemicals has been acq.. |
|||
Viscosity | 20 cP | 20 cP | |
Lord Adhesives 7713 Adhesion Increaser to SMC Lord Adhesion Enhancers/Surface ModifiersTo meet the unique bonding demands that accompany the use of difficult-to-bond materials, the Lord Corporation offers a full line of adhesion enhancers/surfa.. |
|||
Viscosity | 20 - 100 cP | 20 - 100 cP | As Supplied |
Heraeus Cleviosâ„¢ PH 510 Conductive Sulfonate Polymer for Antistatic Coatings Poly(3,4-ethylenedioxythiophene)poly(styrenesulfonate), provided as an aqueous dispersion used to produce thin film antistatic coatings. Cleviosâ„¢ PH 510 is an antistatic material based on PEDO.. |
|||
Viscosity | 20 cP @Temperature 25.0 °C |
20 cP @Temperature 77.0 °F |
|
Silikony Polskie Polsil OM 20 Methyl Silicone Fluid The methyl silicone fluids are liquid organic silicone polymers, including inorganic elements (Si-O bond, as in quartz, glass or sand) and inorganic elements (methyl groups) in one molecule. This gi.. |
|||
Viscosity | 20 cP | 20 cP | |
Solvay CATAFOR® MS/T Surfactant Description: Proprietary blendIdentification: ALKALI METAL SALT IN SOLVENTSoluble in polar organic solvent. Soluble in water.pH: NeutralAvailable in: Asia Pacific, Europe, Latin America and North Am.. |
|||
Viscosity | 20 cP | 20 cP | |
Solvay DURAPHOS® TLP Tri lauryl phosphite Chemical Name: TRIALKYL PHOSPHITECAS: 68610-62-8; 108-95-2 Available in: Asia Pacific, Europe, Latin America and North AmericaWater Solubility: Practically Insoluble Applications: DURAPHOS® TLP i.. |
|||
Viscosity | 20 - 30 cP @Temperature 25.0 °C |
20 - 30 cP @Temperature 77.0 °F |
Mixed |
Trelleborg Emerson & Cuming Eccobond® 23 LV General Purpose Catalyst Emerson & Cuming 23 LV Eccobond® General Purpose CatalystExcellent low temperature performance properties, excellent thermal shock/cycle and impact resistance. Good hardener for cryogenic applicati.. |
|||
Viscosity | 20 cP | 20 cP | Dynamic |
Dow Corning SYL-OFF® PMCPSL 11 Crosslinker This Syl-Off ® Crosslinker is one component of a multi-component silicone release coating system. In order to use this product effectively, it must be blended with the appropriate Syl-Off ® coatin.. |
|||
Viscosity | 20 cP | 20 cP | dynamic |
Dow Corning TM-1951 EMULSION Dow Corning® TM-1950 Emulsion and Dow Corning® TM-1951 Emulsion are water-based silicone products with excellent dilution stability, which provide release of tissue paper from felt, fabric and wir.. |
|||
Viscosity | 20 cP | 20 cP | Apparent |
CIMBAR Suspengel™ 325 Plus High Purity Bentonite, Industrial Grade Suspengel products are manufactured from the highest quality Western Bentonite reserves. Suspengel products are easy to disperse thixotropes with excellent suspension properties. Strict process co.. |
|||
Viscosity | 20 - 55 cP | 20 - 55 cP | |
Beijing Ranger Chem B-63 Liquid Epoxy Resin Information provided by Beijing Ranger Chemical Co. |
|||
Viscosity | 20 cP | 20 cP | |
Asahi Glass Fluon® AD1 PTFE Aqueous Dispersion Fluon®PTFE aqueous dispersions are useful for glass cloth coating, metal coating, binder, additive in resin, feedstock of heat resistive paint ,etc.Information provided by Asahi Glass Company, Inc... |
|||
Viscosity | 20 cP | 20 cP | |
3M Scotch-Weld™ CA40 Instant Adhesive 3M™ Scotch-Weld™ Instant Adhesives are single component, high strength cyanoacrylate adhesives. Very fast setting and excellent adhesion to many substrates including flexible vinyl and EPDM rubbe.. |
|||
Viscosity | 20 cP @Temperature 20.0 °C |
20 cP @Temperature 68.0 °F |
|
Solvay Specialty Polymers Diofan® A 736 Polyvinylidene Chloride (PVDC)
(Unverified Data**) DIOFAN® A 736 is a PVDC latex used as a flexible underlayer for coating on paper, cardboard and rigid PVC foils, to be covered with an appropriate topcoat.Additional Information: PROCESSING - DRYIN.. |