Material Notes:
Fomblin® PFPE fluorinated lubricants are used when harsh chemical environments, high temperatures or wide working-temperature ranges are encountered.Information provided by Solvay Solexis, Inc.
Physical Properties Metric English Comments
Density 1.86 g/cc
0.0672 lb/in³
ASTM D891
Viscosity Measurement 236
236
Viscosity Index; ASTM D2270
Kinematic Viscosity 153 cSt

@Temperature 20.0 °C
153 cSt

@Temperature 68.0 °F
ASTM D445
Kinematic Viscosity at 40°C (104°F) 72 cSt
72 cSt
ASTM D445
Kinematic Viscosity at 100°C (212°F) 16 cSt
16 cSt
ASTM D445
Molecular Weight 4500 g/mol
4500 g/mol
Evaporation Loss 14 %
14 %
22 hrs. at 204°C; ASTM 2595
Mechanical Properties Metric English Comments
Four Ball Extreme Pressure, Weld Load 102 kg
225 lb (mass)
Mean Hertz Load; IP 239
316 kg
697 lb (mass)
Init. Seiz. Load; IP 239
398 kg
878 lb (mass)
Welding Load; IP 239
Four Ball Wear 0.700 mm
0.0276 in
Avg. scar diameter; ASTM D4172
Thermal Properties Metric English Comments
Pour Point -68.0 °C
-90.4 °F
ASTM D97