Material Notes:
Description: Flame retardant polyamide PA6 reinforced with mineral filler, for injection molding.Available in: Asia Pacific, Europe, Latin America and North America Product Applications: This phosphorus and halogen free flame retardant grade is particularly suitable for equipment with robust glow wire resistance such as MCB housings. This grade is available in grey color.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.37 g/cc
0.0495 lb/in³
ISO 1183/A
Mechanical Properties Metric English Comments
Tensile Strength at Break 35.0 MPa
5080 psi
ISO 527 Type 1A
Tensile Strength, Yield 35.0 MPa
5080 psi
ISO 527 type 1 A
Elongation at Break 12.2 %
12.2 %
ISO 527 Type 1A
Elongation at Yield 18.2 %
18.2 %
ISO 527 type 1 A
Tensile Modulus 2.50 GPa
363 ksi
ISO 527 Type 1A
Flexural Strength 56.0 MPa
8120 psi
ISO 178
Flexural Modulus 2.30 GPa
334 ksi
ISO 178
Charpy Impact Unnotched 6.00 J/cm²
28.6 ft-lb/in²
ISO 179/1eU
Charpy Impact, Notched 0.580 J/cm²
2.76 ft-lb/in²
ISO 179/1eA
Processing Properties Metric English Comments
Moisture Content <= 0.20 %
<= 0.20 %