Material Notes:
Description: TECHNYLSTAR polyamide, reinforced with 35% of glass fiber, for injection molding. Characterized by a high fluidity of the melt.Available in: Europe and North AmericaProduct Applications: Due to its outstanding flow characteristics, TECHNYLSTAR TM S 216 V35 provides a significant productivity improvement and allows more freedom in mould design and part design versus standard polyamide solutions. This product is available in natural.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.41 g/cc
0.0509 lb/in³
ISO 1183/A
Water Absorption 0.90 %

@Temperature 23.0 °C,
Time 86400 sec
0.90 %

@Temperature 73.4 °F,
Time 24.0 hour
ISO 62
Mechanical Properties Metric English Comments
Tensile Strength at Break 195 MPa
28300 psi
ISO 527 Type 1A
Elongation at Break 3.0 %
3.0 %
ISO 527 Type 1A
Tensile Modulus 10.7 GPa
1550 ksi
ISO 527 Type 1A
Flexural Strength 295 MPa
42800 psi
ISO 178
Flexural Modulus 10.0 GPa
1450 ksi
ISO 178
Izod Impact, Notched (ISO) 13.0 kJ/m²
6.19 ft-lb/in²
ISO 180/1eA
Izod Impact, Unnotched (ISO) 75.0 kJ/m²
35.7 ft-lb/in²
ISO 180/1eU
Charpy Impact Unnotched 7.50 J/cm²
35.7 ft-lb/in²
ISO 179/1eU
Charpy Impact, Notched 1.30 J/cm²
6.19 ft-lb/in²
ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 222 °C
432 °F
ISO 11357
Flammability, UL94 HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in
1210
Glow Wire Test 650 °C

@Thickness 1.60 mm
1200 °F

@Thickness 0.0630 in
ISO 60695-2-12
Processing Properties Metric English Comments
Feed Temperature 220 - 225 °C
428 - 437 °F
Front Barrel Temperature 235 - 245 °C
455 - 473 °F
Mold Temperature 80.0 °C
176 °F
Drying Temperature 80.0 °C
176 °F
Moisture Content <= 0.20 %
<= 0.20 %
Descriptive Properties Value Comments
Compression Zone 225-235°C