Spartech E65060 General Purpose PVC

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer Spartech
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Spartech E65060 General Purpose PVC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
First choice for compounds meeting the stringent requirements of Spiral Hose, Automotive, Housewares, Farm Equipment, Coated Fencing and numerous other applications including Lawn & Garden Wheels. Best for clear tubing, profiles, and co-extrusion.Information provided by Spartech
Physical Properties Metric English Comments
Specific Gravity 1.17 g/cc
1.17 g/cc
+.02
Mechanical Properties Metric English Comments
Hardness, Shore A 60
60
10 sec ± 3
Tensile Strength, Yield 11.0 MPa
1600 psi
Elongation at Break 470 %
470 %
100% Modulus 0.00407 GPa
0.590 ksi
Processing Properties Metric English Comments
Melt Temperature 154 °C
310 °F