Spartech PP7110 Talc Filled High Impact Copolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 10% Talc Filler
Manufacturer Spartech
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Spartech PP7110 Talc Filled High Impact Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Good material choice for applications where low to medium levels of impact are required and where stiffness and heat deflection properties remain criticalInformation provided by Spartech
Physical Properties Metric English Comments
Specific Gravity 0.960 g/cc

@Temperature 22.8 °C
0.960 g/cc

@Temperature 73.0 °F
ASTM D792
Filler Content 10 %
10 %
Linear Mold Shrinkage 0.018 cm/cm
0.018 in/in
0.125inch wall
Mechanical Properties Metric English Comments
Tensile Strength, Yield 22.1 MPa
3200 psi
ASTM D638
Elongation at Break >= 400 %
>= 400 %
ASTM D638
Elongation at Yield 12 %
12 %
ASTM D638
Flexural Modulus 1.10 GPa
160 ksi
secant; ASTM D790
1.38 GPa
200 ksi
tangent; ASTM D790
Izod Impact, Notched >= 5.34 J/cm

@Temperature 22.8 °C
>= 10.0 ft-lb/in

@Temperature 73.0 °F
ASTM D256
Gardner Impact >= 33.9 J

@Temperature 22.8 °C
>= 25.0 ft-lb

@Temperature 73.0 °F
ASTM D5420
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 90.6 °C
195 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 46.1 °C
115 °F
ASTM D648
Optical Properties Metric English Comments
Gloss 55 %
55 %
60°; ASTM D523
Users viewing this material also viewed the following: