Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 90.6 °C | 195 °F | ASTM D648 |
RheTech Products FT3150-01 Thermoplastic Polyolefin, Non-UV Stabilized, Black Applications: Air deflectorsUnderhood componentsBumper componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 90.6 °C | 195 °F | ASTM D648 |
RheTech Products FT4900-01UV Thermoplastic Polyolefin, UV Stabilized, Black Applications: Exterior componentsBodyside moldingsStep padsLicense plate bracketsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 90.6 °C | 195 °F | ASTM D648 |
RheTech Products FT4900-745UV Thermoplastic Polyolefin, UV Stabilized, CJM Medium Khaki Solid Applications: Exterior componentsBodyside moldingsStep padsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 90.6 °C | 195 °F | ASTM D648 |
RheTech Products FT4900-746UV Thermoplastic Polyolefin, UV Stabilized, CD7 Dark Slate Solid Applications: Exterior componentsBodyside moldingsStep padsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 90.6 °C | 195 °F | ASTM D648 |
RheTech Products FT4900-772UV Thermoplastic Polyolefin, UV Stabilized, RXF Jet Black Applications: Exterior componentsBodyside moldingsStep padsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 90.6 °C | 195 °F | ASTM D648 |
RheTech Products FT5250-650UVA Thermoplastic Polyolefin, UV Stabilized, Exterior 848 Black Applications: Cowl vent grillesExterior componentsBodyside moldingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 90.6 °C @Thickness 3.18 mm |
195 °F @Thickness 0.125 in |
Unannealed; ASTM D648 |
PolyOne Maxxam™ PPH-20C UV Natural Polypropylene Homopolymer (PP Homopolymer) PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 90.6 °C | 195 °F | ASTM D648 |
RheTech Products P249-01UV General Purpose Polypropylene Copolymer, UV Stabilized, Black Applications: LP bracketsSplash shieldsDoor/trunk scuffInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 90.6 °C | 195 °F | ASTM D648 |
RheTech Products UVP254-01 Polypropylene Copolymer, UV Stabilized, Black Applications: Fuel filler pocketInterior trimI/P componentsCenter consoleInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 90.6 °C | 195 °F | ASTM D648 |
Polymer Resources PC/TP-FR2 Flame Retardant PC/Polyester Alloy Flame Retardant, High Impact, Excellent Chemical ResistanceFeatures: • Flame Retardant • Impact Modified • Self Extinguishing • Good Chemical ResistanceProcess: Injection MoldingNotes: All p.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 90.6 °C | 195 °F | ASTM D648 |
Polymer Resources PC/ABS-FR1-[color]-UV Flame Retardant PC/ABS Alloy, UV-stabilized PC/ABS Alloy, Flame Retardant, Standard Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Infor.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 90.6 °C | 195 °F | ASTM D648 |
Ineos H01H-00 Polypropylene Homopolymer This is a low flow rate homopolymer designed for extrusion or injection molding. This material meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520.Applic.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 90.6 °C | 195 °F | ASTM D648 |
Ineos H04G-00 Polypropylene Homopolymer This is a controlled rheology general purpose homopolymer polypropylene. This grade is designed to meet the processing and physical property requirements of film and profile extrusion applications... |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 90.6 °C | 195 °F | ASTM D648 |
Ineos R12C-00 Polypropylene Random Copolymer Grade R12C-00 is a high clarity, medium flow rate random copolymer with low antistat for injection molding and stretch blow molding applications. This material meets the requirements of the U.S. Foo.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 90.6 °C | 195 °F | (0.250"); ASTM D648 |
LTL Color Compounds ColorRxâ„¢ PP2-1002AF Food Grade Polypropylene Random Copolymer An approx. 10 melt Polypropylene random copolymer with FDA food contact approval and antimicrobial protection.All information provided by LTL Color Compounders, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 90.6 °C | 195 °F | (0.250"); ASTM D648 |
LTL Color Compounds ColorRxâ„¢ PP2-1002ARX Biocompatible Polypropylene Random Copolymer A biocompatible approx. 10 melt injection molding grade of Polypropylene random copolymer for healthcare applications.All information provided by LTL Color Compounders, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 90.6 °C | 195 °F | (0.250"); ASTM D648 |
LTL Color Compounds ColorRxâ„¢ PP2-1002ARX Biocompatible, Antimicrobial Polypropylene Random Copolymer A biocompatible( approx. 10 melt Polypropylene random copolymer for healthcare applications containing antimicrobial protection.All information provided by LTL Color Compounders, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 90.6 °C | 195 °F | (0.250"); ASTM D648 |
LTL Color Compounds ColorRxâ„¢ PP2-1005ARX Biocompatible, Antimicrobial Polypropylene Random Copolymer A biocompatible approx. 10 melt Polypropylene random copolymer for healthcare applications, containing a high level of antimicrobial protection for FDA regulated medical devices.All information prov.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 90.6 °C | 195 °F | ASTM D648 |
Spartech PP7110 Talc Filled High Impact Copolymer Good material choice for applications where low to medium levels of impact are required and where stiffness and heat deflection properties remain criticalInformation provided by Spartech |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 90.6 °C | 195 °F | ASTM Test |
Styrolution Terblend® N NM-11 ABS/PA6 (Dry) Terblend N NM-11 is an ABS/PA6 blend combining very high impact strength, even at low temperatures, with an excellent processability and surface appearance.Information provided by STYROLUTION, which.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 90.6 °C | 195 °F | Unannealed; ASTM D648 |
Styron MAGNUMâ„¢ 342 EZ Acrylonitrile Butadiene Styrene (ABS) Resin Overview: MAGNUMâ„¢ 342 EZ ABS resin is a medium impact, high flow, low gloss resin often used in automotive applications. Automotive MAGNUM ABS resins offer a wide range of gloss, viscosity, imp.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 90.6 °C | 195 °F | ASTM D648 |
A. Schulman PP 1259 Polypropylene Medium Impact Polypropylene DescriptionPolypropylene PP 1259 is a medium impact polypropylene with easier molding characteristics for thinner parts and longer flow distances. Lower molding pressures and heats often reduce war.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 90.6 °C | 195 °F | ASTM D648 |
A. Schulman PP 1259 Polypropylene Medium Impact Polypropylene DescriptionPolypropylene PP 1259 is a medium impact polypropylene with easier molding characteristics for thinner parts and longer flow distances. Lower molding pressures and heats often reduce war.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 90.6 °C | 195 °F | ASTM D648 |
Washington Penn Medium Impact Copolymer 20% Calcium Carbonate Filled Calcium carbonate-filled polypropylene compounds have been tailored specifically to meet the requirements of each of the major automobile producers. Grades are available to meet FDA food and drug pa.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 90.6 °C | 195 °F | ASTM D648 |
A. Schulman PP 1259 Polypropylene Medium Impact Polypropylene DescriptionPolypropylene PP 1259 is a medium impact polypropylene with easier molding characteristics for thinner parts and longer flow distances. Lower molding pressures and heats often reduce war.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 90.6 °C | 195 °F | ASTM D648 |
A. Schulman PP 1259 Polypropylene Medium Impact Polypropylene DescriptionPolypropylene PP 1259 is a medium impact polypropylene with easier molding characteristics for thinner parts and longer flow distances. Lower molding pressures and heats often reduce war.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 90.6 °C | 195 °F | ASTM D648 |
A. Schulman PP 1259 Polypropylene Medium Impact Polypropylene DescriptionPolypropylene PP 1259 is a medium impact polypropylene with easier molding characteristics for thinner parts and longer flow distances. Lower molding pressures and heats often reduce war.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 90.6 °C | 195 °F | ASTM D648 |
Americas Styrenics STYRON A-TECH® 1170 High Impact Polystyrene Product CharacteristicsGood impact resistanceConsistent colorabilityEasy processingFood Contact CompliantUL Classification 94HBTypical ApplicationsExtruded SheetSmall AppliancesRefrigeration Accesso.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 90.6 °C | 195 °F | ASTM D648 |
Aaron Industries AVPP C 200-2 MELT 30 Clarified Virgin Polypropylene A natural polypropylene copolymer resin specifically designed for injection molding applications - containing clarifiers. |