Material Notes:
A copper-nickel alloy designed for specialized electrical and electronic applications. It has a very low temperature coefficient of resistance and medium-range electrical resistivity. Used for wire-wound precision resistors and bi-metal contacts. Standard product forms are strip and wire.Data provided by the manufacturer, Special Metals.
Physical Properties Metric English Comments
Density 8.89 g/cc
0.321 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 441 MPa
64000 psi
Annealed
Tensile Strength, Yield 134 MPa

@Strain 0.200 %
19400 psi

@Strain 0.200 %
Annealed
Elongation at Break 51 %
51 %
Annealed
Thermal Properties Metric English Comments
CTE, linear 13.7 µm/m-°C

@Temperature 20.0 - 100 °C
7.61 µin/in-°F

@Temperature 68.0 - 212 °F
Thermal Conductivity 19.2 W/m-K
133 BTU-in/hr-ft²-°F
Component Elements Properties Metric English Comments
Carbon, C <= 0.10 %
<= 0.10 %
Copper, Cu 54 %
54 %
As remainder
Iron, Fe <= 0.75 %
<= 0.75 %
Manganese, Mn <= 2.25 %
<= 2.25 %
Nickel, Ni 40 - 45 %
40 - 45 %
Including Cobalt
Silicon, Si <= 0.25 %
<= 0.25 %
Sulfur, S <= 0.015 %
<= 0.015 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000489 ohm-cm
0.0000489 ohm-cm
Temperature coefficient of resistance is +/-36 µOhm/Ohm-°C in the range 25-150°C.
Curie Temperature <= -196 °C
<= -321 °F
Users viewing this material also viewed the following: