Material Notes:
Terblend N NM-13 is a new experimental ABS/PA6-Blend with improved impact strength at low temperatures. It can be easily processed on any standard injection molding machine.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS.
Physical Properties Metric English Comments
Melt Flow 13 g/10 min

@Load 10.0 kg,
Temperature 240 °C
13 g/10 min

@Load 22.0 lb,
Temperature 464 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 35.0 MPa
5080 psi
50mm/min; ISO 527
Elongation at Break >= 50 %
>= 50 %
50mm/min, Nominal strain; ISO 527
Tensile Modulus 1.60 GPa
232 ksi
1mm/min; ISO 527
Charpy Impact, Notched 8.00 J/cm²
38.1 ft-lb/in²
ISO 179
5.50 J/cm²

@Temperature -30.0 °C
26.2 ft-lb/in²

@Temperature -22.0 °F
ISO 179
Thermal Properties Metric English Comments
Vicat Softening Point 91.0 °C
196 °F
(50 °C/h / 50N) - B/50; ISO 306
Descriptive Properties Value Comments
Commercial Status Active America
Primary Processing Technique Injection Molding
UL.UL-C Yes