Styron CALIBREâ„¢ 301-58 LT Polycarbonate Resin

Category Polymer , Thermoplastic , Polycarbonate (PC)
Manufacturer Styron
Trade Name CALIBRE™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Styron CALIBREâ„¢ 301-58 LT Polycarbonate Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Overview: CALIBREâ„¢ 301-58 LT is a high light transmission, high-flow polycarbonate resin for injection molding applications.Main Characteristics:High light transmissionHigh flow for injection moldingHigh purityApplications:LED opticsLight guidesInformation provided by Styron
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
ISO 1183/B; ASTM D792
Water Absorption 0.20 %

@Temperature 23.0 °C,
Time 86400 sec
0.20 %

@Temperature 73.4 °F,
Time 24.0 hour
ISO 62
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm
0.0050 - 0.0070 in/in
ISO 294-4
Melt Flow 58 g/10 min

@Load 1.20 kg,
Temperature 300 °C
58 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength at Break 48.0 MPa
6960 psi
ISO 527-2/50
Tensile Strength, Yield 60.0 MPa
8700 psi
ISO 527-2/50
Elongation at Break 60 %
60 %
ISO 527-2/50
Elongation at Yield 6.0 %
6.0 %
ISO 527-2/50
Tensile Modulus 2.30 GPa
334 ksi
ISO 527-2/50
Flexural Strength 100 MPa
14500 psi
2.0 mm/min; ISO 178
Flexural Modulus 2.50 GPa
363 ksi
2.0 mm/min; ISO 178
Izod Impact, Notched (ISO) 58.0 kJ/m²

@Temperature 23.0 °C
27.6 ft-lb/in²

@Temperature 73.4 °F
ISO 180/4A
Izod Impact, Unnotched (ISO) NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
ISO 180
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 137 °C
279 °F
Annealed; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 124 °C
255 °F
Unannealed; ISO 75-2/A
134 °C
273 °F
Annealed; ISO 75-2/A
Vicat Softening Point 147 °C
297 °F
ISO 306/B50
Optical Properties Metric English Comments
Refractive Index 1.583
1.583
ISO 489
Haze 1.0 %
1.0 %
ASTM D1003
Transmission, Visible >= 90 %
>= 90 %
ASTM D1003