Material Notes:
CALIBREâ„¢ 7100-15 glass-reinforced resin offers increased modulus and improved heat distortion resistance, with minimal shrinkage. It also offers outstanding UL-94 flammability ratings. CALIBREâ„¢ 7100-15 additive package: No mold release.Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010.
Physical Properties Metric English Comments
Density 1.27 g/cc
0.0459 lb/in³
ISO 1183B
Linear Mold Shrinkage, Transverse 0.0020 - 0.0050 cm/cm
0.0020 - 0.0050 in/in
ISO 294-4
Melt Flow 15 g/10 min

@Load 1.20 kg,
Temperature 300 °C
15 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 57.0 MPa
8270 psi
50 mm/min; ISO 527-2
Tensile Strength, Yield 60.0 MPa
8700 psi
50 mm/min; ISO 527-2
Elongation at Break 6.0 %
6.0 %
50 mm/min; ISO 527-2
Elongation at Yield 4.0 %
4.0 %
50 mm/min; ISO 527-2
Tensile Modulus 3.50 GPa
508 ksi
ISO 527
Izod Impact, Notched 0.950 J/cm
1.78 ft-lb/in
ISO 180/A
Charpy Impact, Notched 0.850 J/cm²
4.05 ft-lb/in²
ISO 179/1eA
Thermal Properties Metric English Comments
Vicat Softening Point 150 °C
302 °F
50°C/hr, 50N; ISO 306-B50
Flammability, UL94 V-0

@Thickness 1.50 mm
V-0

@Thickness 0.0591 in
5VA

@Thickness 3.00 mm
5VA

@Thickness 0.118 in
Ring & Ball Softening Point >= 125 °C
>= 257 °F
IEC 60335-1
Electrical Properties Metric English Comments
Comparative Tracking Index 175 V
175 V
IEC 60112
Users viewing this material also viewed the following: