Material Notes:
Product CharacteristicsExtrusion GradeHeat ResistantInformation provided by Calsak Corporation
Physical Properties Metric English Comments
Specific Gravity 1.19 g/cc
1.19 g/cc
ASTM D792
Linear Mold Shrinkage 0.0020 - 0.0060 cm/cm
0.0020 - 0.0060 in/in
ASTM D955
Melt Flow 2.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
2.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 71.7 MPa
10400 psi
ASTM D638
Elongation at Yield 13 %
13 %
ASTM D638
Tensile Modulus 3.17 GPa
460 ksi
ASTM D638
Flexural Yield Strength 120 MPa
17400 psi
ASTM D790
Izod Impact, Notched 0.422 J/cm

@Thickness 3.17 mm,
Temperature 22.8 °C
0.790 ft-lb/in

@Thickness 0.125 in,
Temperature 73.0 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 104 °C

@Thickness 3.17 mm
219 °F

@Thickness 0.125 in
annealed; ASTM D648
Vicat Softening Point 116 °C
241 °F
ASTM D1525
Optical Properties Metric English Comments
Refractive Index 1.49
1.49
ASTM D542
Haze 0.50 %
0.50 %
ASTM D1003
Transmission, Visible 93 %
93 %
Total light Transmission; ASTM D1003