Thermal Properties Metric English Comments
Vicat Softening Point 116 °C
241 °F
Rate B/50; ISO 306
SABIC Innovative Plastics Cycolac® INP630 ABS
INP630 is a specialty polymer that increases the service temperature of products. Can be used with a impact modifier to provide impact strength as well as high heat resistance. Provides excellent hi..
Vicat Softening Point 116 °C
241 °F
Rate B/120; ISO 306
SABIC Innovative Plastics Cycoloy® CX1440 PC+ABS
CYCOLOY CX1440 is a general purpose PC+ABS blend specially developped for thin wall applications requiring weld line strength and high flow with a good balance of properties
Vicat Softening Point 116 °C
241 °F
Rate B/120; ISO 306
SABIC Innovative Plastics Cycoloy® CX1440 PC+ABS (Europe-Africa-Middle East)
CYCOLOY CX1440 is a general purpose PC+ABS blend specially developped for thin wall applications requiring weld line strength and high flow with a good balance of propertiesThis data was supplied by..
Vicat Softening Point 116 °C
241 °F
Rate B/120; ISO 306
SABIC Innovative Plastics Lexan® BX9349 PC COPOLYMER (Asia Pacific)
Lexan* BX9349 resin is an injection moldable modified PC resin with non-brominated and non-chlorinated flame retardant to meet UL-94 V0 at 0.5mm and V2 at 0.4mm. Balanced flow with low temperature d..
Vicat Softening Point 116 °C
241 °F
ASTM D1525
Reliance Industries Reclair R35042 Polyethylene
Rotational molding Medium Density Polyethylene grade. Characteristics:good toughness, good impact resistance, good environmental stress crack resistance. Applications:chemical tanks, water storage ..
Vicat Softening Point 116 °C
241 °F
50°C/hr; 50N
Polimeri Europa KOBLEND HI 41 F1 PBT+PC, Impact Grade  (discontinued **)
Symbol according to ISO 1043/1: PBT+PC-HI Similar to KOBLEND HI 41 with improved fluidity. Main application fields: bumpers Unfilled. Suitable for Injection Molding. Supplied as pellets.ISO data..
Vicat Softening Point 116 °C
241 °F
VST/B/50; ISO 306
GEHR Plastics PP-30PET-F Polypropylene, 30% PET Fiber Reinforced  (discontinued **)
Polypropylene shows a high mechanical strength and a tensile strength, but a low notched impact strength. PP resists stress cracking and it is easy to weld. At minus temperatures it can get brittle...
Vicat Softening Point 116 °C
241 °F
Rate B/120; ISO 306
SABIC Innovative Plastics Cycoloy® C1000HF PC+ABS (Europe-Africa-Middle East)
CYCOLOY C1000HF is a general purpose PC+ABS blend specially developed for thin wall applications requiring a high flow with a good balance of properties. It is suitable for applications in the autom..
Vicat Softening Point 116 - 216 °C
241 - 421 °F
Average value: 148 °C Grade Count:16
Overview of materials for Polyphenylene Ether, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, Molded". Each property range of values reported is minimum and maximum values of ap..
Vicat Softening Point 116 °C
240 °F
120°C/h, 50 N; ASTM D1525
Polymer Resources ABS-GP-HH General Purpose ABS, High Heat
General Purpose Acrylonitrile Butadiene Styrene, High HeatProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform..
Vicat Softening Point 116 °C
241 °F
ASTM D1525
LyondellBasell Alathon® H4262 High Density Polyethylene, Injection Molding Grade  (discontinued **)
ApplicationsAlathon H4262 is a high-flow resin that exhibits very good cold temperature impact performance, optimum processing and thermal stability, with good color and organoleptic properties. Typ..
Vicat Softening Point 116 °C
241 °F
Rate B/50; ISO 306
SABIC Innovative Plastics Lexan® SLDM310 PC (Asia Pacific)
Mineral filled Antistatic Polycarbonate, HDT110degC type
Vicat Softening Point 116 - 124 °C
241 - 255 °F
Average value: 121 °C Grade Count:6
Overview of materials for Medium Density Polyethylene (MDPE), Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "Medium Density Polyethylene (MDPE), Film Grade". Each property range of values reported is minimum and m..
Vicat Softening Point 116 °C
241 °F
(Ring and Ball) ASTM E28
LyondellBasell Montell 0800 Polybutene
Key Features: highly isotactic, semi-crystalline homopolymer, good creep resistance, good environmental crack resistance, miscible with polypropylenes, FDA acceptableApplications: concrete carrierMe..
Vicat Softening Point 116 °C
241 °F
ASTM D1525
LyondellBasell Alathon® H4250 High Density Polyethylene, Injection Molding Grade
ALATHON H4250 is a high-flow “freezer” grade resin that exhibits enhanced cold temperature impact performance, enhanced processing and thermal stability, with good color and organoleptic p..
Vicat Softening Point 116 °C

@Load 5.00 kg
241 °F

@Load 11.0 lb
50°C/h; ASTM D1525
LG Chemical LG709W ABS, Low Gloss, Heat Resistance
Injection Molding, Low Gloss, Heat ResistanceApplication: Automobiles Interior Housing (Column Cover, Pilllars, Etc.)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9003-54-7Information provided by LG..
Vicat Softening Point 116 °C
241 °F
Rate B/120; ISO 306
SABIC Innovative Plastics Xenoy® CL500U PBT+PC (Europe-Africa-Middle East)
XENOY CL500U is a semi-crystalline blend, developed for exterior automotive parts ( except bumper shells ) and non automotive parts, requiring good impact, excellent chemical resistance and UV stabi..
Vicat Softening Point 116 °C

@Load 5.10 kg
241 °F

@Load 11.2 lb
50°C/h; ISO 306
Styrolution Novodur® 4115 ABS
Novodur Ultra 4115 is a PC modified high heat injection molding grade. It provides good heat resistance combined with high impact strength.Information provided by Styrolution
Vicat Softening Point 116 °C
241 °F
Rate B/120; ISO 306
SABIC Innovative Plastics Noryl NH3060 PPE+HIPS
NH3060 resin is a modified PPE + PS blend with an excellent balance of non-chlorinated non-brominated flame retardance, hydrolytic stability, impact and heat resistance, good flow, and low specific ..
Vicat Softening Point 116 °C
241 °F
Rate B/120; ISO 306
SABIC Innovative Plastics NORYL EXNL0353 PPE+HIPS
EXNL0353 resin is a modified PPE + PS blend with an excellent balance of non-halogenated flame retardance, hydrolytic stability, impact and heat resistance, good flow, and low specific gravity for l..
Vicat Softening Point 116 °C
241 °F
Rate B/50; ASTM D1525
SABIC Innovative Plastics NORYL PVX0901 PPE+PS (Asia Pacific)
Multi purpose V1 grade
Vicat Softening Point 116 °C
241 °F
ASTM D1525
PlastxWorld CEVIAN®-V 400T ABS
Heat Resistant ABSThese are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc.
Vicat Softening Point 116 °C
241 °F
ASTM D1525
Westlake MC2001 High Density Polyethylene Coating
Westlake MC2001 is a high density polyethylene designed for extrusion coating and lamination applications. MC2001 provides improved barrier properties, temperature resistance, stress crack resistanc..
Vicat Softening Point 116 °C
241 °F
A50; ISO 306
Lubrizol ESTANE® 58133 Ester Based Thermoplastic Polyurethane (European Grade)
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability ..
Vicat Softening Point 116 °C
241 °F
50°C/h 50N; ISO 306
Covestro Bayblend® FR 3011 Polycarbonate + ABS, Flame Retardant Grade
Injection molding gradegood flowhigh heat resistanceVicat/B 120 temperature = 118 °CUL-listing 94 V-0 (1.5 mm) antimony-, chlorine- and bromine-free flame retardantglow wire test (GWFI): 960 °..
Vicat Softening Point 116 °C
241 °F
ASTM D1525
Dow DFDC-7525 NT High Density Polyethylene Resin
DOW DFDC-7525 NT is produced using UNIPOL™ process technology. It is intended for use in thin wall drip tape and micro-irrigation tube, hose and tube, and profile extrusion applications. Informati..
Vicat Softening Point 116 °C
241 °F
ASTM D1525
Dow TUFLIN™ HS-7065 NT 7 Linear Low Density Polyethylene Resin
Hexene Linear Low Density Resin Good Processability at Narrow Die Gaps Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a TUFLIN™ HS-7065 NT 7 is a fractional melt, ethylene-hexene copolymer, designe..
Vicat Softening Point 116 °C
241 °F
Rate B/120; ISO 306
SABIC Innovative Plastics Cycoloy® CX1440 PC+ABS (Asia Pacific)
CYCOLOY CX1440 is a general purpose PC+ABS blend specially developped for thin wall applications requiring weld line strength and high flow with a good balance of properties
Vicat Softening Point 116 °C
241 °F
ASTM D1525
Dow PELLETHANE® 2103-75D Film Grade Thermoplastic Polyurethane Elastomer  (discontinued **)
Description: PELLETHANE® 2103-75D UV stabilized, polyether based thermoplastic polyurethane elastomer has excellent hydrolytic stability and excellent resistance to micro-organisms. Applications in..
Vicat Softening Point 116 °C
241 °F
ISO 306
Unipetrol PE HD LITEN® VL 29 HDPE
Extrusion and pipe applications.Information provided by Unipetrol RPA