Suzhou Hipro Polymers Hiprolon® 200 NN Nylon 1010, conditioned

Category Polymer , Renewable/Recycled Polymer , Thermoplastic , Nylon
Manufacturer Suzhou Hipro Polymers
Trade Name Hiprolon®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Suzhou Hipro Polymers Hiprolon® 200 NN Nylon 1010, conditioned.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Hiprolon® 200 NN is a medium viscosity polyamide 10,10 with neat resin based on bio-renewable resource. It features low density, low water absorption, good cold impact resistance, good wear-resistance and flow ability. It is widely used as neat resin for compounding, general injection molding process, tubing or film extrusion, powder coating, et al.Information provided by Suzhou Hipro Polymers Co. Ltd
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0376 lb/in³
ISO 1183
Water Absorption 0.70 %
0.70 %
ISO 62
Mechanical Properties Metric English Comments
Tensile Strength, Yield 50.0 MPa
7250 psi
ISO 527-1/-2
Elongation at Break >= 50 %
>= 50 %
ISO 527-2/1A
Tensile Modulus 1.50 GPa
218 ksi
ISO 527-1/-2
Flexural Modulus 1.20 GPa
174 ksi
ISO 178
Charpy Impact Unnotched NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
ISO 179/1eU
NB

@Temperature -30.0 °C
NB

@Temperature -22.0 °F
ISO 179/1eU
Charpy Impact, Notched 0.800 J/cm²

@Temperature -30.0 °C
3.81 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
1.10 J/cm²

@Temperature 23.0 °C
5.23 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 202 °C
396 °F
ISO 11357