TIMCAL TIMREX® SFG10 Primary Synthetic Graphite

Category Carbon , Graphite , Other Engineering Material , Additive/Filler for Polymer
Manufacturer TIMCAL
Trade Name TIMREX®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF TIMCAL TIMREX® SFG10 Primary Synthetic Graphite.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all production and processing stages, strict final inspection, and clearly defined development processes.TIMREX Primary Synthetic Graphite shows unique properties thanks to the combination of a consistent purity, perfect crystalline structure and well defined texture.Information provided by TIMCAL
Physical Properties Metric English Comments
Bulk Density 0.0700 g/cc
0.00253 lb/in³
Scott
Particle Size 9.0 - 15.5 µm
9.0 - 15.5 µm
d90, Guaranteed
12.8 µm
12.8 µm
d90, Typical
Ash 0.070 %
0.070 %
Typical
<= 0.10 %
<= 0.10 %
Guaranteed
Processing Properties Metric English Comments
Moisture Content 0.10 %
0.10 %
Typical
<= 0.50 %
<= 0.50 %
Guaranteed
Descriptive Properties Value Comments
Aspect Fine black powder
Crystallinity, Lc, nm >150
Interlayer Distance, nm .3354-.3358